Dittos to all what Dwight said. . Seal bagging will prevent oxidation only. If warpage occurs during assembly, it can be corrected. Many boards are mounted in such a way that will make them flat. As long as warpage is within limits, it's fine. On the other hand, boards that need to slide into a card cage have to be straight or very little warpage, much less than the limits.
Regards,
Ramon.
> -----Original Message-----
> From: Dwight Mattix [SMTP:[log in to unmask]]
> Sent: Wednesday, May 05, 2004 1:54 PM
> To: [log in to unmask]
> Subject: Re: [TN] Raw Card warpage
>
> At 12:09 PM 5/5/2004 -0500, Victor G. Hernandez wrote:
> >Fellow TechNetters,
> >
> > At a PWB factory setting is a final baking process permissible to
> >correct any warpage prior to customer shipment.
>
> Some customers allow it or do not specify either way. Some customers
> specify against it. If not specified either way then tacit approval for
> "flat baking" is generally assumed to be given.
>
> >Once the sealed bag is
> >open and product not used for an extended period of time will the
> >warpage return.
>
> Not necessarily. It will only rewarp if the pwb design is unbalanced
> (either in dielectric stackup or in metal pattern distribution). An
> unbalanced design will (re)warp to some degree when heated during solder
> assembly.
>
> Dwight Mattix
> Sr Staff QE, Corp Eng
>
> >Victor G. Hernandez
> >
> >---------------------------------------------------
> >Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> >To unsubscribe, send a message to [log in to unmask] with following text in
> >the BODY (NOT the subject field): SIGNOFF Technet
> >To temporarily halt or (re-start) delivery of Technet send e-mail to
> >[log in to unmask]: SET Technet NOMAIL or (MAIL)
> >To receive ONE mailing per day of all the posts: send e-mail to
> >[log in to unmask]: SET Technet Digest
> >Search the archives of previous posts at: http://listserv.ipc.org/archives
> >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> >for additional information, or contact Keach Sasamori at [log in to unmask] or
> >847-509-9700 ext.5315
> >-----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|