Joe,
I have used ARMAKLEEN E-2003 and had no problems with it when I worked at
Hydor-Aire in Burbank California. SCAQMD has no problems other than you can
not discharge the water waste, but require that you recycle the waste water.
Quoting "Macko, Joe @ IEC" <[log in to unmask]>:
> Good Morning,
>
> Another potential line stopper has appeared on the horizon. My production
> supervisor notified me that the Ecosolve saponifier made by AlphaMetals is
> no longer available. We have a WESTEK in-line cleaner that uses Ecosolve to
> clean RMA flux residue from boards. We are also located in Southern
> California so we have stringent drainage and air quality (VOC emission)
> rules that need to be considered.
>
> Does anyone have any excess EcoSolve they would like to sell to get us
> through this transition?
>
> Has anyone faced this same problem and switched from EcoSolve to another
> aqueous cleaner to remove RMA flux residue and no clean?
>
> AlphaMetal's is recommending their ARMAKLEEN E-2003 as a replacement for
> Ecosolve. Anyone out there using ARMAKLEEN that would like to comment on
> its performance on RMA (and no-clean)?
>
> Can anyone recommend a southern California consultant that could help us
> transition to another cleaning agent?
>
>
> thanks
> joe
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|