Yep, I agree that soldering brass is hairy and, quite often, we still
see brass components (tinned or nude) without any barrier layer. Believe
it or not, I've even seen brass components which were 2 µm thick
electrolytically hard-gold-plated (solder-in sockets) without a barrier
layer :-(
Brian
Bob willis wrote:
> Just comment again on a similar tac I would like to hear from suppliers
> on what they are doing on barrier plating on brass terminals. People I
> have spoken too seen to missing this and the problems associated with
> soldering to brass. Copper is often used as a barrier layer and nickel.
> If copper is being used how much more is being plated to overcome the
> copper dissolution and then the complete non wetting.
>
> Some time back a well known contributor to this forum made the point
> that they had failures.
>
>
> Bob Willis
> 2 Fourth Ave, Chelmsford,
> Essex, CM1 4HA, England
> Tel: 01245 351502
> Fax: 01245 496123
> Mobile: 07860 775858
> Email: [log in to unmask]
> Web: www.leadfreesoldering.com
> Web: www.bobwillis.co.uk
>
>
> -----Original Message-----
> From: Leadfree [mailto:[log in to unmask]] On Behalf Of Kim Rappard
> Sent: 10 May 2004 23:55
> To: [log in to unmask]
> Subject: [LF] FW: Re: Using Brass for interconnections
>
> Our product has an electronic controller, in some instances we use brass
> nuts and washers for terminating from our loom to various electrical
> circuits such as elements.
>
>
>
> The (RoHS) directive States "Lead as an alloying element in steel
> containing up to 0,35 % lead by
>
> weight, aluminium containing up to 0,4 % lead by weight and as a copper
> alloy containing up to 4 % lead by weight"
>
>
>
> Brass is not covered in the directive!
>
>
>
> Brass usually contains lead for machining.
>
> Does this mean we are unable to use brass as an electrical conductor?
>
>
>
>
>
> Kim Rappard
> Electronics Development Engineer
>
>
> Main Number +64 (3) 363 9293
> Direct Dial +64 (3) 363 9515
> Fax +64 (3) 363 9294
> <mailto:[log in to unmask]>
> <mailto:[log in to unmask]> [log in to unmask]
> <mailto:[log in to unmask]>
>
> 224 Armagh Street
> PO Box 13-705
> Christchurch
> NEW ZEALAND
>
> www.whispergen.com
>
> _____
>
> Important: This electronic mail message and any attachments are
> confidential and may be legally privileged. If you are not the intended
> receipient, you may not legally copy, disclose or use the contents in
> any way, and you should contact me immediately and destroy this message.
> Thank you.
>
> _____
>
>
>
>
> ------------------------------------------------------------------------
> -------Leadfee Mail List provided as a service by IPC using LISTSERV
> 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Leadfree
> To temporarily stop delivery of Leadree for vacation breaks send: SET
> Leadfree NOMAIL
> Search previous postings at: http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> ------------------------------------------------------------------------
> -------
>
> -------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Leadfree
> To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
> Search previous postings at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -------------------------------------------------------------------------------
>
>
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-------------------------------------------------------------------------------
|