Hi Chuck and IPC LF Listservers,
Thanks,
I had to go look up the source documents since this was interesting.
I didn't see them in the original posting.
Kelley, M., Watson, P., Thorton, D., and Halpin, T. J. Lead intoxication
associated with chewing plastic wire coating. Morbidity and Mortality
Weekly Report 42:465-467. 1993
http://www.cdc.gov/mmwr/preview/mmwrhtml/00020984.htm
It was interesting how turnertoys came up highest on my intial search.
http://www.turnertoys.com/PVC_framepage1.htm
http://www.greenpeaceusa.org/media/publications/lead/reftext.htm
Was listed in another search
--------------------------------
Actually it doesn't surprise me that the electrical worker would do
something like this, nor that it would be a great unforseen.
I bet, I bet, no one fully communicated this study to all the effected
workers or hobby people.
When we go fully Lead Free WE, are going to have similar unforseens.
YiEngr, MA/NY DDave
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-------------------------------------------------------------------------------
|
|
|