I'd like to offer a TI application note which shows board level soldering performance with SnPb, NiPd, and NiPdAu finished components soldered using SnPb(Ag) and SnAgCu solders.
You can access this paper by clicking the link titled "Evaluation of Nickel/Palladium/Gold-Finished Surface-Mount Integrated Circuits (July 2001)" on the following page:
http://focus.ti.com/quality/docs/gencontent.tsp?templateId=5909&navigationId=11219&path=templatedata/cm/ecoinfo/data/leadfree_appnotes
Best regards,
Doug Romm, MGTS
[log in to unmask]
Texas Instruments
Phone: 903 868-7388; Fax: 903 868-6002
US mail: M/S 812, PO Box 84; Sherman, TX 75091
Shipping: 6412 Hwy 75 South, Sherman, TX 75090
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]]On Behalf Of santhakumar
rajesnayagham
Sent: Thursday, May 06, 2004 10:49 AM
To: [log in to unmask]
Subject: [LF] reliability study on SAC with various PCB and component
finish combinations
Hi All,
Has anybody performed reliability studies on the following combination?
Solder paste: SAC (any combination)
PCB finish: Immersion Silver or Immersion Tin
Component finish: any lead-free finish is ok
for a variety of components?
Thank you,
Sincerely,
Santhakumar
Fern Abrams <[log in to unmask]> wrote:Just to clarify, IPC filed comments with the EU Technical Adaption
Committee regarding the need for clarification proposed definition of
LF:
"A maximum concentration value of 0.1% by weight in homogeneous
materials
for lead, mercury, hexavalent chromium, polybrominated biphenyls (PBB)
and
polybrominated diphenyl ethers (PBDE) and of 0.01% weight in homogeneous
materials for cadmium shall be tolerated. Homogeneous material means a
unit
that can not be mechanically disjointed in single materials".
While I have had no formal response, we have heard informally that this
is unlikely to be further clarified and may end up being settled in
court.
Fern Abrams
Director of Environmental Policy
IPC - The Association Connecting Electronics Industries
1333 H Street, NW, 11th Floor West
Washington, DC 20005
(202) 962-0460
fax (202) 962-0464
www.ipc.org
-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Wednesday, May 05, 2004 4:49 PM
To: [log in to unmask]
Subject: Re: [LF] Lead in resistors
Gordon,
No, not very comforting.
The IPC Materials Declaration Team has sent a letter to the appropriate
EU personnel asking for clarification of some of these issues, but to
the best of my knowledge Fern has still not received an answer. This is
probably because they (EU) had not thought that far ahead when they
drafted the dreadful thing in the first place. As more than one wag has
stated, we will probably have to wait for clarification when that first
unfortunate company is dragged into court. Then we MIGHT get definitive
answers.
regards,
Bev Christian
Research in Motion
-----Original Message-----
From: Davy, Gordon [mailto:[log in to unmask]]
Sent: May 5, 2004 4:26 PM
To: [log in to unmask]
Subject: Re: [LF] Lead in resistors
Bill Haas has noted that 0402 surface-mount "lead-free" resistors were
found to contain more than 1000 ppm Pb, and that the suppliers assured
him that this is OK per the RoHS legislation. Bill wanted to know where
it says in the directive that what the resistor manufacturers told him
is so. Annex item 7 exempts Pb in "electronic ceramic parts (e.g.
piezoelectronic devices)", so it looks as if this is what they are
referring to.
What the Directive doesn't say anywhere, of course, is that for
components not exempted by the Annex the maximum allowable level is 1000
ppm, or how the limit (whatever it turns out to be) is to be calculated
- i.e., what is to be used as the fraction denominator: termination
finish, component as a whole, assembly as a whole, equipment as a whole.
Article 4 paragraphs 1 and 2 say that there can't be any Pb at all
except per the Annex, and paragraph 3 puts manufacturers on notice that
they may have to eliminate other stuff later.
Also not spelled out is how users of components - such as Bill - are
expected to document that the equipment items that they are selling are
Pb-free: will the envirocops be satisfied if the equipment manufacturer
can produce upon demand a certificate of compliance from the
manufacturers of each component? If not, how diligent does the original
equipment manufacturer have to be to ensure that no Pb above the
to-be-determined limit (except as permitted by the Annex) has crept into
his product?
As an analogy, hardware destined for space has long had a prohibition
against pure tin plating. Yet every time a satellite has been audited,
cases of pure tin plating have been found, due simply to human error.
Can you imagine the jeopardy of the manufacturer of an electronic
system, wondering if a particular item will be randomly selected to find
out if it contains Pb? (X-ray fluorescence will be useless for levels of
1000 ppm, so if that's the level that is finally chosen, we're talking
serious chemical analysis.)
Article 8 specifies that the penalties are to be "effective,
proportionate, and dissuasive." I don't see any language describing how
disagreements are to be resolved, or what happens to the equipment while
the matter is being settled. Not very comforting.
Gordon Davy
Baltimore, MD
[log in to unmask]
410-993-7399
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d To unsubscribe, send a message to [log in to unmask] with following
text in the BODY (NOT the subject field): SIGNOFF Leadfree To
temporarily stop delivery of Leadree for vacation breaks send: SET
Leadfree NOMAIL Search previous postings at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
-------
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d To unsubscribe, send a message to [log in to unmask] with following
text in the BODY (NOT the subject field): SIGNOFF Leadfree To
temporarily stop delivery of Leadree for vacation breaks send: SET
Leadfree NOMAIL Search previous postings at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
-------
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-------------------------------------------------------------------------------
Santhakumar Rajesnayagham
Graduate Student & Research Assistant
Center for Electronics Manufacturing and Assembly (CEMA)
Rochester Institute of Technology, Rochester, New York
Phone : (CEMA Lab) 585-475-7293
---------------------------------
Do you Yahoo!?
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-------------------------------------------------------------------------------
Win a $20,000 Career Makeover at Yahoo! HotJobs
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-------------------------------------------------------------------------------
|