Bill,
Nickel only? Yikes! Yes, I have heard of it and have been at the painful end of a supplier providing parts with a nickel only finish. What a nightmare. Avoid at all costs!! There is a very good reason why ENIG is ENIG and not EN! Nickel oxidizes quite nicely, thank you very much.
Bev Christian
Research in Motion
-----Original Message-----
From: William E. Hunt [mailto:[log in to unmask]]
Sent: May 4, 2004 3:37 PM
To: [log in to unmask]
Subject: [LF] LF PWB finish
I have been working with some fabricators in Asia and I'm looking for some
outside input.
What LF finishes are recommended for a low cost consumer products A and B
(see below)?
Product A: Currently XPC with HASL and has a contact switch on board. OSP
not compatible.
Product B: Currntly XPC with HASL - no contact switch
What is the advantages and disadvantages each finish?
Anyone heard of Ni plating (no gold)?
Thanks,
Bill
Bill Hunt
OTUC Engineering
Eastman Kodak
Office: 585-726-4892
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-------------------------------------------------------------------------------
Fax: 585-726-3278
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-------------------------------------------------------------------------------
|
|
|