Dave:
The report has been updated, substantially. Some of this was reported at
IPC last year and is on our website at:
http://www.tycoelectronics.com/environment/leadfree/pdf/Tyco_IPC_2003_Chou.p
df
More to come...
Cheers,
Bob
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]]On Behalf Of MA/NY DDave
Sent: Friday, May 28, 2004 12:44 PM
To: [log in to unmask]
Subject: Re: [LF] Lead Free design guides for press fit
Hi Cemco-Peter, Tyco-Hilty and IPC LF Listservers,
I have been striving to stay off list to do other LF study and work yet
this is an exciting proposition for technical information. As you know I
still have a NIST duty to negotiate / reclaim and a few others.
First of all this report that Bob linked us to now and in the past, is done
quite well.
The European Tyco group did a great job of giving the baseline for SnPb HAL
or HASL yet I guess were not able to do comparatives for all the other
metallurgies. I mean sometimes studies just are not complete yet can still
be done really well.
So I hope you can all negotiate and can find the time to update this fine
report by Belgium, Tyco
Yours in Engineering, Dave
Y i Engr, MA/NY DDave
On Fri, 28 May 2004 15:06:34 +0100, Pete Lymn <[log in to unmask]> wrote:
>Thanks Robert,
>I read the paper with interest but note that fused lead free solders were
>not compared. Lead free solders can be applied using adapted HASL machines
>and result in more uniform surface and hole coatings. The lighter alloys
>require less energy to level resulting in a much tighter thickness range
>with improved 'minimum' thicknesses and significantly lower 'maximum'
>thicknesses. Hole clearing is more uniform with less closedown. If you or
>anyone else would like us to tin some sample to compare please do not
>hesitate to contact me. We have SnCu+Ni permanently available and will be
>conducting trials with two SAC alloys in the next few weeks...
>Peter.
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET
Leadfree NOMAIL
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
---
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-------------------------------------------------------------------------------
|
|
|