Marie, we typically use the IPC class 2 spec for our products, but on
occasion have to trim leads to fit into off the shelf enclosures. We have
many thousands of devices in the field with leads clipped into the solder
meniscus itself. All of our television metering equipment cycles back
through our repair center and to my knowledge, we've never had any
significant failures due to solder fracture when clipping leads. Still it's
not something we like to do and is only done when absolutely necessary. I
think if your vendor is using a Q cutter or hand trimming using sharp
cutters you're probably OK, but I still cringe. If ya have to, ya have to.
Bob Croslin
Nielsen Media Research
-----Original Message-----
From: Dobbs, Marie [mailto:[log in to unmask]]
Sent: Friday, May 28, 2004 10:20 AM
To: [log in to unmask]
Subject: [TN] Through hole components question
Just Wondering.. Through Hole Assembly
Do Most Contract Manufacturers have "Component Prep Departments" that
receive all their comps and the detape them, form them(bend), hand prep with
crimps, and Cut the leads short for loose hand assembly. Does anyone out
there cut the leads after soldering. I know that IPC says this is not a
good practice,,, but ...
Thanks in advance for feedback
Marie A. Dobbs
Training and Development Specialist
Tyco Safety Products
100 Technology Drive
Westminster, MA 01473
Phone: 1-978-731-6827
Fax: 1-978-731-6950
email: [log in to unmask]
In any moment of decision the best thing you can do is the right thing, the
next best thing is the wrong thing, and the worst thing you can do is
nothing."
Theodore Roosevelt
26th President of the United States
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|