Theoretically, there should be no difference at all, as the manufacturing
system is supposed to be the same, but the difference will be in the
"acceptance" of the product at inspection stages including finals. The
testing (mechanical and electrical) could be different ie 1 x 260oC as
opposed to 6 x 288oC solder shock, but this is customer spec'd and should
reflect the type of materials used higher tg etc.
The nature of application changes, which determines the testing and
acceptance regime(flying boards etc/environmentally challenging) but visual
attributes could slacken for non-sensitive applications such as white goods,
where say for instance an "orange peel" resist finish would not detract from
the working properties of the PWB, or measling where seen would not stop the
function of the PWB.
Regards,
Colin McVean
Circuit Manufacture Ltd
Unit 9-12
Rowleys Green Lane
Longford
Coventry
CV6 6AG
Tel: 02476 666168
Fax: 02476 637089
________________________________________________
This email is confidential and intended solely for the use
of the individual to whom it is addressed. Any views or
opinions presented are solely those of the author and do
not necessarily represent those of the Company.
If you are not the intended recipient, be advised that you
have received this email in error and that any use,
dissemination, forwarding, printing, or copying of this
email is strictly prohibited.
If you have received this email in error please notify the
Company by telephone on +44 (0)24 7666 6168 or reply
by email to the sender and delete the email.
________________________________________________
Whilst every effort has been made to ensure that there are
no viruses embedded in this email, we highly recommend
that you virus scan any attached files using your own anti-
virus software.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Franklin
Sent: 25 May 2004 15:54
To: [log in to unmask]
Subject: Re: [TN] Visual Acuity
I'll concede I missed something there, now help me out with this thought,
what do you believe the "processing" differences are between a Class II
product, and 55110 product?
Franklin
----- Original Message -----
From: "Blair K. Hogg" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, May 25, 2004 9:10 AM
Subject: Re: [TN] Visual Acuity
Franklin,
I think you missed Brian's point somewhat.
The easiest way to increase the cost of a product is to over-specify its
requirements.
Should the components of a portable radio be processed to the same standards
as those of military flight hardware? The portable radio will most likely
never see the environments that military flight hardware will see, although
I'll admit that a portable radio can see some pretty nasty environments,
e.g., sand, salt atmosphere (at the beach), vibration (bouncing around in
the back of a truck), etc. We would expect the portable radio to survive
these environments, but its failure would not be life-threatening. Do we
really want to build product that long outlasts its useful life?
I agree that we should always strive to make our products better, and less
costly if possible, but then we have to start to get into business
strategies and product placement in the market, etc.
Products should be specified correctly for their application and for the
customer's needs. Anything above that generally adds cost.
Blair
>>> [log in to unmask] 05/25/04 09:48AM >>>
Wow, that was off topic...but since a new one is started let me add this...
1. Specifications are here to stay, period.
2. They must be adhered to, period.
3. There are many ways of adhering to most specifications, many ways cost
more than others, most specifications can be met by applying different, more
cost effective methods than what is 'traditionaly' performed.
4. Instead of cutting back on 'meeting specifications' for non-military
product, why not develop cost effective processes so that military and
non-military product are processed in a similar manner at the lowest cost
possible. From my perspective, the only real difference between the military
and non-military product are the additional tests required, and those cost's
are typically passed on to the customer anyway.
Franklin
----- Original Message -----
From: "Brian Ellis" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, May 25, 2004 1:38 AM
Subject: Re: [TN] Visual Acuity
> Jack
>
> Interesting point, but an analogic argument can be applied to all those
> who apply rigid standards where they are not necessary. If a product,
> process or whatever does what it should do in an acceptable manner with
> appropriate aids provided by the employer, then that is good enough. I
> firmly believe that our industry is plagued by over-specification-itis.
> This is often engendered by ignorance; a responsible person has no idea
> what the ramifications of a process or product are so, instead of
> learning what it does, he covers his ignorance by applying
> specifications and standards, often irrelevant or far too severe, and
> costing his employers an arm and a leg in consequence. I see many, many
> examples of this in this forum, as well as visiting clients. In one
> company which consulted me, the product was a range of cards for use in
> ordinary PCs used in an office environment. I saved them ~40% of their
> production costs and thereby increased their overall gross profitability
> by ~10% simply by showing them that they did not have to build their
> products to ultra-reliable military standards -- but it was a hard
> battle convincing them.
>
> I suggest that every manufacturing entity should carefully examine their
> products and processes for over-specification-itis.
>
> Sorry to diverge off-topic.
>
> Brian
>
> Jack Crawford wrote:
> > Any related requirements have been or are being removed from IPC
> > standards. The correct assessment is whether an individual can do the
> > job they are required to do in an acceptable manner with appropriate
> > aids that may need to be provided by the employer. For broader
> > explanation, i.e. avoiding worker discrimination lawsuits, consult your
> > HR about the Americans with Disabilities Act.
> >
> > Jack Crawford
> > Director, Certification and Assembly Technology
> > [log in to unmask]
> > 847-790-5393
> > fax 847-504-2393
> >
> >
> > -----Original Message-----
> > From: Mary Jane Chism [mailto:[log in to unmask]]
> > Sent: Monday, May 24, 2004 2:37 PM
> > To: [log in to unmask]
> > Subject: [TN] Visual Acuity
> >
> >
> > Group,
> >
> > Is it mentioned anywhere in any of the IPC standards a visual acuity for
> > solder inspection? Thanks.
> >
> > Mary Jane Chism
> >
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following text
> > in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
> > http://listserv.ipc.org/archives
> > Please visit IPC web site
> > http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> > ext.5315
> > -----------------------------------------------------
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following text
in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
http://listserv.ipc.org/archives
> > Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> > -----------------------------------------------------
> >
> >
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3..16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
*******************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they
are addressed. If you have received this email in error please notify
the system manager.
This footnote also confirms that this email message has been swept
for the presence of computer viruses.
www.hubbell.com - Hubbell Incorporated
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|