Nan Ya Plastics makes a high(er) resin content 7628- 50% RC.
http://www.npc.com.tw/Emd-e/e-di1/OK03.html is a direct link to their data sheet page.
Isola makes a 7628 with 47% RC. (IS450)
And to answer Bill's first (and second?) question, high resin content is opposed to what is considered standard or normal. The RC of 7628 is around 40% (IPC-2222, Table 4-2). Nan Ya makes a medium resin content 7628 of 47% and an "LF" type that is 43%, besides their "standard" and "high" types.
I'm sure somebody has the answer as to how resin content affects board construction. I know of the surface flatness/finish (complements of Jeff Bush) issue, but I'm sure there are more.
Best Regards,
Roger M. Stoops, CID+
Trimble Navigation Ltd., Dayton, OH, USA
Ph: +01 937.245.5288
Fax: +01 937.233.7511
p.s.: I'm not a materials expert, let alone anything else... I jus' connect the dots...
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Brooks,Bill
Sent: Tuesday, May 18, 2004 3:50 PM
To: [log in to unmask]
Subject: [TN] FW: [DC] Core Constructions
Is there a materials expert out there that can answer Mike's question below?
B-stage epoxy resin is somewhat of a mystery to many designers. Perhaps
someone can clarify the reference to "High Resin Content" as apposed to ?
what other options are available and how they affect the construction of the
FR4 board. Please copy to the group too so we can all learn from this.
Bill Brooks
PCB Design Engineer , C.I.D., C.I.I.
Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
http://pcbwizards.com
-----Original Message-----
From: Mike Valle [mailto:[log in to unmask]]
Sent: Tuesday, May 18, 2004 12:24 PM
To: [log in to unmask]
Subject: [DC] Core Constructions
Hi, I need some help trying to find some information on FR-4
construction and thickness. I've come across a 4-layer stackup on a
cross-section detail on one of our drawings and I can't seem to find it
in IPC-4121. Our b-stage construction calls out for 1 ply of b-stage
HRC (high resin content) 7628 .0068.
Another detail on another drawing calls out for 1 ply of b-stage HRC
(high resin content) 7628 .008. What I've been finding in IPC-4121 is
that there is a FR-4 11 (7.087) 7628 40% RC and a HFR-4 11 (7.087) 40%
RC, which is a high tg. So, my question is - is there such a thing as
HRC - high resin content with varying thicknesses?
Thanks,
Mike Valle
Project Engineer, PCB Design
Shure Inc.
(847)424-4616
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|