Hi Tom:
Pretinning makes the stranded wire not flexible and easier to break off at the end of the tinned area. We do not pretin any crimped contacts for this very reason.
Regards,
Ramon
-----Original Message-----
From: Tom Gervascio [mailto:[log in to unmask]]
Sent: Wednesday, May 12, 2004 9:54 AM
To: [log in to unmask]
Subject: [TN] Wire crimping
We have an application where we think we are forming galvanic corrosion between silver plated wire and exposed copper (from mechanical stripping). One suggestion that we had was to permit us to pretin the wire with a ROL0 halide free flux, water wash and then crimp on the mating part. The response I received was "In response to question 1. No. Stranded wire must not be tinned when using crimped contact.
There are two reasons I'm aware of: 1. The crimp would not hold properly. 2.
Tinning stranded wire makes it brittle. Brittleness is not an issue at the
CCA end of this wire because it gets potted, but the crimp-connector end is
subjected to movement and vibration. "
Any feedback on this- the application is an high reliability avionics application and must conform to IPC-A-610 Class 3. I would think that pretinning the wire would effectively distribute any forces over a larger cross sectional area (the solder would wet between the individual stands of wire). I would think that pretinning would not make the wire brittle but the downside I could think of- 1.making sure that all flux residues are out of the joint,
2. the insulation is not damaged by the pretinning,
3. and increasing the resistance of the interconnection
Any information would be appreciated.
Tom Gervascio
Senior Process Engineer
Sparton Electronics
(352) 540-4040
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|