All -
Please reference the following link for the exact specifications related to
the part we are dealing with - specifically pages 98 and 99
http://download.micron.com/pdf/datasheets/dram/ddr2/256Mb_x4x8x16_DDR2_B.pdf
I have a handful of parts that I need to reball; however, we don't have any
in-house micro BGA stencils that will accommodate this component. In the
middle of the underside of the part, there is a ridge that prevents a
stencil from laying flat against the surface - this ridge extends up to 8
mils beyond the base of the package. So, I will need a special stencil.
Does anyone out there have any experience with these components? Any ideas
or suggestions? Potentially a lead where I can have a stencil purchased
that will conform to the underside of this part?
I'm still new to the BGA game - so forgive me. If there is additional
information needed, just let me know.
I appreciate the help.
Thanks.
Dacia Leanne Schoolfield
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------