We're talking with our customers about converting from
RMA to an ORH1 water soluble flux for wave soldering. We've
completed qualification testing per J-STD-001, but they have
some questions.
We'll be cleaning with an in-line system right after wave.
Before conformal coat, we plan to clean 100% in a batch system
with 75% isopropanol and DI water. Sump resistivity is
monitored, so we will be performing 100% ROSE test on each lot.
Customer wonders what happens if there is any WSF residue at
all left on the boards between the time they are cleaned with the
in-line and the final cleaning stage. Allowing time for hand soldering
and Genrad test, this is usually a day or two, but in the extreme, it
could be weeks.
They have the impression that WSF residues are strongly
corrosive, and the boards could turn to mush. We have a
board that was soldered in November and hasn't been cleaned,
and solder joints are still shiny.
Question is this - any known instances of corrosion happening
in an air-conditioned shop?
Joe Kane
BAE SYSTEMS Controls
Johnson City, NY
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|