TECHNET Archives

May 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
"Howard A. Cyker" <[log in to unmask]>
Date:
Mon, 24 May 2004 17:21:02 -0400
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (65 lines)
Russ,

Source Electronics in NH (603-595-2906) should be able to do this work for
you.  I don't think that you should have to necessarily re-tin the leads if
they are baked in a Nitrogen atmosphere.    You can try a solderability
test to confirm.

Howard A. Cyker
Senior Manufacturing Engineer
SynQor, Inc.
E-mail:  [log in to unmask]




                      Russ Nowland
                      <[log in to unmask]        To:       [log in to unmask]
                      COM>                     cc:
                      Sent by: TechNet         Subject:  [TN] Component Rework
                      <[log in to unmask]>


                      05/24/2004 04:29
                      PM
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to Russ
                      Nowland






I have several QFP's that have reached beyond their reasonable shelf life.
Many of these components are obsolete and therefore I have to be able to
solder them.  Does anybody know a reliable source that can bake and rework
the surface finish, and re-dry pack them.  The majority of the parts are
Sn/Pb.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2