TECHNET Archives

May 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Thu, 13 May 2004 08:59:40 +0100
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
<002201c438bf$70ddce70$0101c80a@mod>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (123 lines)
Possibly very long times over liquidus could be contributing/aggravating
dewetting conditions. However I would not expect properly applied HASL
finish to dewet if exposed to 230C. The fact that you are using VPR as a
heat source, and SN96 on the other side of the PCB is not really germane.

In fact in the absence of solderability test equipment a pretty good test
for solderability for Sn63 finished boards would be to reflow them fluxless
in an inert atmosphere at around 230C and visually inspect for pull back and
poor wetting....... 

Regards 

Mike Fenner 
Indium Corporation 
NEW: LEAD-FREE European Seminar
http://quickstart-de.register.indium.net/

T: + 44 1908 580 400
M: + 44 7810 526 317 
F: + 44 1908 580 411 
E: [log in to unmask] 
W: www.indium.com 
Pb-free: www.Pb-Free.com 



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ido Mashall
Sent: 13 May 2004 08:54
To: [log in to unmask]
Subject: Re: [TN] Reflow problem


to me it sounds like a difference in the melting temperature.
HASL is usually 67/33 Sn/Pb with lower melting point than your paste SN96.
when heating to get soldering to the high temperature paste all the HASL
become a fluid
what result in the situation you mentioned.
to my opinion you will need to ask for different HASL with higher Tg or
other class of PWB finish. e.g. silver for
that kind of paste.

best regards,

Ido Mashall
----- Original Message -----
From: "Jason W. Gregory" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, May 12, 2004 2:26 PM
Subject: [TN] Reflow problem


> Hello all,
>
> After running a single pass of a double sided SMT board, the bottom side
> solder from HASL is spiking and pooling up in the middle of the pad (from
> gravity), forcing us to wick and prep the side prior to running the
bottom.
> You can actually see the copper showing lightly around the edges of the
> pads. We are running vapor phase reflow and the solder paste used is SN96
> (high temp soldering). Has anyone seen this? I am leaning towards profile
> issues. However, I wanted to see if anyone has seen this and if it was fab
> issues or not.
>
>
> TIA,
>
> Jason Gregory
> Manufacturing Engineer
> LaBarge Inc. --- Houston
> (281)207-1464
> (281)207-1435 fax
> (832)724-0076 cell
> [log in to unmask]
> http://www.labarge.com
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------


:::::::::::::::::::::::::::

This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.

:::::::::::::::::::::::::::

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2