Hi Brian - one of the fundamental rules of galvanic couples that most of us
learned many moons ago but continually forget (although you remembered!)
is to keep the anode-to-cathode ratio as large as possible - which per your
description is already a favorable ratio. IMHO your use environment is hot,
dry and pretty benign for most of the year - I would make sure that the
panel design has minimal moisture trapping/pooling configuration and not do
much else. The use of paint and/or an adhesive to limit environmental
exposure is another fundamental rule but given your use environment may be
overkill. How much electricity are you going to be able to generate?

Dave Hillman
Rockwell Collins
[log in to unmask]



                                                                       
                      Brian Ellis                                      
                      <b_ellis@PROTONIQ        To:       [log in to unmask]
                      UE.COM>                  cc:                     
                      Sent by: TechNet         Subject:  [TN] Slightly OT for conformal coating experts.
                      <[log in to unmask]>                                
                                                                       
                                                                       
                      04/06/2004 09:31                                 
                      AM                                               
                      Please respond to                                
                      "TechNet E-Mail                                  
                      Forum."; Please                                  
                      respond to Brian                                 
                      Ellis                                            
                                                                       
                                                                       





I'm on the point of ordering a solar panel installation. The PV panels
are set into an aluminium profile framework, held together with
stainless steel (presumably 18/8 alloy) screws etc. The installation has
a projected lifetime of ~40 years. In this timeframe, I'm a wee bittie
worried about dissimilar metals, exposed to the weather, causing
corrosion. Granted the surface area of the Al is ginormous, compared to
that of the hardware, so that the corrosion will not be localised.

The weather here is typically 9 months hot and dry (say, 25 - 47°C, 45 -
20% RH resp.), aggravated by direct exposure to the sunlight. The other
three months are cool with intermittent heavy rain (say, 0 - 25°C, 45%++
RH).

Would it help to paint onto the hardware (not the profiles) an epoxy
coating, after the screws have been tightened, to reduce the risk of
long-term corrosion? If so, what type? How does the epoxy stand up to UV
exposure over the years?

TIA

Brian

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2