I'm on the point of ordering a solar panel installation. The PV panels
are set into an aluminium profile framework, held together with
stainless steel (presumably 18/8 alloy) screws etc. The installation has
a projected lifetime of ~40 years. In this timeframe, I'm a wee bittie
worried about dissimilar metals, exposed to the weather, causing
corrosion. Granted the surface area of the Al is ginormous, compared to
that of the hardware, so that the corrosion will not be localised.
The weather here is typically 9 months hot and dry (say, 25 - 47°C, 45 -
20% RH resp.), aggravated by direct exposure to the sunlight. The other
three months are cool with intermittent heavy rain (say, 0 - 25°C, 45%++
RH).
Would it help to paint onto the hardware (not the profiles) an epoxy
coating, after the screws have been tightened, to reduce the risk of
long-term corrosion? If so, what type? How does the epoxy stand up to UV
exposure over the years?
TIA
Brian
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|