Get whoever is asking for "3 oz. copper" to state the thickness they
desire in inches - there will be confusion if that doesn't happen and most
likely the end result won't be right. If the requirement is stated in
inches, it can be checked by cross-section of representative holes in a
coupon. Also, make them aware that the surface plates up at a higher rate
in the hole; do they also want "thick" copper on the surface or just the
holes? That will dictate how you approach the plating process; as someone
said: button plate if the traces are not also thick. If the traces also
need to be thick copper, make sure they are wide with good spacing between
features; and that the tolerance on width goes up proportionately. One
last thought: the holes need to be over-drilled so that you can "fit" all
that copper; so make sure that the pads and clearances are adequate.
Valerie
"Victor G. Hernandez" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
04/26/2004 09:07 AM
Please respond to "TechNet E-Mail Forum."; Please respond to
Victor_G_Hernandez
To: [log in to unmask]
cc:
Subject: Re: [TN] Stack-up for 2 layer, 3oz. copper board
Susan,
Check IPC-A-600F p. 73 for Starting and process Foil Thickness.
Then you can calculate plated copper thickness in barrel.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Susan Mansilla
Sent: Monday, April 26, 2004 6:46 AM
To: [log in to unmask]
Subject: Re: [TN] Stack-up for 2 layer, 3oz. copper board
Just a little technical issue that concerns me - when people give a
plating deposit in the hole or even on the surface in oz. - what exactly
do they need and how do you measure it.
In the IPC specs we have thickness values that are to be met when
starting with a specific foil weight but we don't have a thickness value
for the statement - 3 oz for the hole wall.
Do you spec a ounce weight on the drawing and expect the thickness to be
in the range of what copper foil would be on laminate?
Susan Mansilla
Robisan Lab
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|