TECHNET Archives

April 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Tom Burek <[log in to unmask]>
Date:
Fri, 9 Apr 2004 09:50:45 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Jeffrey Bush <[log in to unmask]>
Parts/Attachments:
text/plain (77 lines)
The surface flatness is really the issue here and somewhere the design
activity picked up from a PC house that they use a fine glass against
the foil layers to ensure good circuit development.  The idea that a
laminate supplier can produce a smoother surface because of lam
technology may be true for some, but not for most.  Good lamination
technologies will product similar surfaces, with differences not large
enough to impact subsequent imaging processes.  We actually see that the
more resin in the package has an adverse impact on stability, which
given the current design technologies has a much higher control priority
than surface geometry from glass type.  A good Copper/Aluminum/Copper
build technology will produce very flat surfaces with all glass styles,
which provide a latitude of build options and package control for the PC
fabricator.



Jeffrey Bush
Director, Quality Assurance and Technical Support

                          76 Technology Drive - POB 1890
                             Brattleboro, Vermont 05302-1890
                                Tel. 802.257.4571.21 Fax. 802.257.0011
                                    [log in to unmask]
                              http://www.vtcircuits.com	



-----Original Message-----
From: Tom Burek [mailto:[log in to unmask]] 
Sent: Thursday, April 08, 2004 4:34 PM
To: [log in to unmask]
Subject: [TN] PCB Laminate/Stackup question


Hello Technetters,
I have a question about layer stack-ups.  Some time ago a respected
contributor to this forum presented us with some valuable information in
the form of a specification he developed.  In this specification, under
the title, MASTER DRAWING NOTES 1.0 Laminate, Core and Prepreg Material,
section 1.9 states,"There shall be no 7628 glass style prepreg used
facing copper. If required, single ply or multi-ply 7628 core material
may be used.  If used as prepreg, 7628 only may be used between two
other more resin rich glass styles." My question is what does this mean
to the stack-up? Why should you not use 7628 facing copper?  Does it
have to do with the amount of resin not present in 7628 and may not bond
to the copper sufficiently?  What should be used? and Why?

I hope this question is not too imposing.

Thank you in advance.

Tom Burek, CID+


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2