hi steve well all the guesses were blaming the board, dendrites, aligmnet,
reisn starvation , but look at the chip in smoking 2 about half way up the
crack on the chip you will see a black burn mark, the chip failed, not the
board, as the chip cracked its usualy a sign it got real hot inside. seen it
many times. if you pull the chip off i bet there is a burn mark under the
chip where it got hot. well thats my guess anyway.
robert Tarzwell
ps they still dont get heavy copper do they i got three emails saying
heavy copper is a dream and does not exist.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|