Brian wouldn't the honey addition also have made a better flux? the sugars
giving a Fehling's like reduction?
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: 27 April 2004 07:11
To: [log in to unmask]
Subject: Re: [TN] Water Soluble Flux For Class 3
Yup! The A version was, I believe, activated with citric and malic acids.
For the record, the makers of the Zeva drag soldering machines
introduced a flux ca. 1975 which also consisted of citric acid,
glycerol, water and ethanol. It wasn't brilliant. I guess they were
particularly fond of tribasic molecules! The Hughes claim of being the
first to use fruit acids was therefore a myth. I dare say that the Zeva
formulation would have made a pleasant cough medecine if they hadn't
been forced to use a denatured alcohol! They should have added some honey!
Brian
Kane, Joseph E wrote:
> We're trying to qualify a water soluble flux, Alpha 3355 HB, for
> wave soldering our military product. We've installed an ultrasonic
> spray fluxer for our wave solder machine, and an in-line aqueous
> cleaner with Vigon A200 in the wash section.
>
> We've performed SIR testing in accordance with J-STD-001C
> Appendix B. We've also done ion chromatography on some
> production boards, some testing with our Omega Meter, and for
> good measure, we conformal coated some samples and ran them
> through ten-day humidity. Everything looks good.
>
> We're not making this change lightly. We think we've done our
> homework, and we've got good equipment and process controls.
> But before we implement, we're reviewing with some of our
> customers, and we're having trouble with one.
>
> Their Objection #1 is that J-STD-001 doesn't permit water soluble
> flux for Class 3. Obviously, that's not how we read it, because
> para. 4.2.b says:
>
> When other activity levels or flux materials are used, data
> demonstrating compliance with testing of Appendix B shall 7
> be available for review.
>
> They get hung up on 4.2.c:
>
> Type H or M fluxes may be used only for tinning of terminals, solid
> wire and sealed components when performed as part of an integrated
> fluxing, soldering, cleaning, and cleanliness test system.
>
> They see "may be used only for tinning..." and stop there. We
> see "may be used only for tinning...when performed as part of..."
> In other words, we think that subparagraph b allows you to qualify
> for soldering per Appendix B, subparagraph c says that if you
> pretin, you must also clean and test.
>
> Their Objection #2 is that nobody else is out there using water
> soluble flux to solder flight-qualified military hardware. We know
> for a fact that this is not true, because we have a sister plant that
> does this, as does one of our competitors just down the road.
>
> First question, a plea really, does anyone have an opinion about
> the intent of J-STD-001C paragraph 4.2?
>
> Second question - who else out there is using water soluble flux
> for Class 3 military? Can you say which flux? Which military
> programs?
>
> I won't use anyone's company name without permission, but I
> need to let our our customer know that we're not trying something
> crazy and without precedent. If we can get beyond that, I think we
> can have meaningful discussion with them about our equipment,
> testing, and process controls.
>
> Joe Kane
> BAE SYSTEMS Controls
> Johnson City, NY
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
:::::::::::::::::::::::::::
This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.
:::::::::::::::::::::::::::
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|