Lance,
The components do have a little bit of a standoff. They are also potted
and the potting is recessed enough that I do believe there is a gap.
The gap may not be big enough to allow for adequate airflow though. So,
I passed this info on to our customer and recommended either a spacer.
Thanks for your help.
-Carrie
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lance Mayes
Sent: Thursday, April 01, 2004 6:04 PM
To: [log in to unmask]
Subject: Re: [TN] Voids in Thru-Hole Solder Joints
Importance: High
Carrie;
First I have a question, is this a hard mount component? If this is the
case it may be that an air pocket is forming below the component body
between the solder and the component.. This type of problem could be
covered in J-STD-001C 6.1.4. What could be done about it, maybe a
spacer or a different prep on the leads such as what we call a cowboy
crimp where the lead is crimped to prevent the component from going all
the way into the through hole. That's what comes to mind as I read your
problem. Hope this or another answer from some more experienced
Technetters help.
Thanks
P. Lance Mayes
Mfg. Trainer
"Morse, Carrie" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
03/31/04 12:11 PM
Please respond to "TechNet E-Mail Forum."; Please respond to "Morse,
Carrie"
To: [log in to unmask]
cc:
Subject: [TN] Voids in Thru-Hole Solder Joints
We recently had circuit card assembly sent out for cross sectioning.
One of the leads for a thru-hole device has voids -- perfectly round
voids. The component body prevents us from seeing the top of the solder
joint (which, if we could have seen, we would have seen a void). The
bottomside of the joint has a void, but, would not have been visible
without cross sectioning. The board was sent out for cross sectioning
to evaluate a different problem, but, cross sectioning was done on a
sample basis to evaluate the entire board. In other words, this
specific component has not been a problem (yet).
My questions are as follows:
1. What causes the voids over the wave? My first guess is insufficient
preheat or dwell time. My second guess is materials (moisture in the
board). Are these valid root causes? What else should I consider?
2. Are the voids detrimental to the reliability of the board? We use
OA flux. I bet there is flux entrapped. That can't be good.
3. What is the acceptance criteria for voids in Thru-Hole parts?
IPC-A-610 sec 6 covers circumferential wetting as well as percent fill
as these are visible without cross sectioning. Is there a spec that
covers what a thru-hole solder joint should look like cross sectioned?
TIA,
Carrie
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|