TECHNET Archives

April 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Tue, 6 Apr 2004 18:38:58 +0300
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-1; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (65 lines)
Thanks, all. I agree the climate here is benign (why do you think that I
chose this place?)

Dave: ~6.55 MWh/year, based on a 3.5 kW nominal installation, 40 m2 of
panels, 340 days with sun, average of 5.5 h/day of "useful" sunshine
(the tourist board always say >2500 h/year, but some of that will be at
queer angles). With government subsidies à la Kyoto Protocol, payback
will be at just over 8 years, even counting interest on the investment.
Of course, whether I'll be alive then is another story (I very much
doubt whether I'll be around for the full 40 years, as that will take me
to a gaga 112!!!!! :-) )

Brian

Brian Ellis wrote:

> I'm on the point of ordering a solar panel installation. The PV panels
> are set into an aluminium profile framework, held together with
> stainless steel (presumably 18/8 alloy) screws etc. The installation has
> a projected lifetime of ~40 years. In this timeframe, I'm a wee bittie
> worried about dissimilar metals, exposed to the weather, causing
> corrosion. Granted the surface area of the Al is ginormous, compared to
> that of the hardware, so that the corrosion will not be localised.
>
> The weather here is typically 9 months hot and dry (say, 25 - 47°C, 45 -
> 20% RH resp.), aggravated by direct exposure to the sunlight. The other
> three months are cool with intermittent heavy rain (say, 0 - 25°C, 45%++
> RH).
>
> Would it help to paint onto the hardware (not the profiles) an epoxy
> coating, after the screws have been tightened, to reduce the risk of
> long-term corrosion? If so, what type? How does the epoxy stand up to UV
> exposure over the years?
>
> TIA
>
> Brian
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2