Yup! The A version was, I believe, activated with citric and malic acids.
For the record, the makers of the Zeva drag soldering machines
introduced a flux ca. 1975 which also consisted of citric acid,
glycerol, water and ethanol. It wasn't brilliant. I guess they were
particularly fond of tribasic molecules! The Hughes claim of being the
first to use fruit acids was therefore a myth. I dare say that the Zeva
formulation would have made a pleasant cough medecine if they hadn't
been forced to use a denatured alcohol! They should have added some honey!
Brian
Kane, Joseph E wrote:
> We're trying to qualify a water soluble flux, Alpha 3355 HB, for
> wave soldering our military product. We've installed an ultrasonic
> spray fluxer for our wave solder machine, and an in-line aqueous
> cleaner with Vigon A200 in the wash section.
>
> We've performed SIR testing in accordance with J-STD-001C
> Appendix B. We've also done ion chromatography on some
> production boards, some testing with our Omega Meter, and for
> good measure, we conformal coated some samples and ran them
> through ten-day humidity. Everything looks good.
>
> We're not making this change lightly. We think we've done our
> homework, and we've got good equipment and process controls.
> But before we implement, we're reviewing with some of our
> customers, and we're having trouble with one.
>
> Their Objection #1 is that J-STD-001 doesn't permit water soluble
> flux for Class 3. Obviously, that's not how we read it, because
> para. 4.2.b says:
>
> When other activity levels or flux materials are used, data
> demonstrating compliance with testing of Appendix B shall 7
> be available for review.
>
> They get hung up on 4.2.c:
>
> Type H or M fluxes may be used only for tinning of terminals, solid
> wire and sealed components when performed as part of an integrated
> fluxing, soldering, cleaning, and cleanliness test system.
>
> They see "may be used only for tinning..." and stop there. We
> see "may be used only for tinning...when performed as part of..."
> In other words, we think that subparagraph b allows you to qualify
> for soldering per Appendix B, subparagraph c says that if you
> pretin, you must also clean and test.
>
> Their Objection #2 is that nobody else is out there using water
> soluble flux to solder flight-qualified military hardware. We know
> for a fact that this is not true, because we have a sister plant that
> does this, as does one of our competitors just down the road.
>
> First question, a plea really, does anyone have an opinion about
> the intent of J-STD-001C paragraph 4.2?
>
> Second question - who else out there is using water soluble flux
> for Class 3 military? Can you say which flux? Which military
> programs?
>
> I won't use anyone's company name without permission, but I
> need to let our our customer know that we're not trying something
> crazy and without precedent. If we can get beyond that, I think we
> can have meaningful discussion with them about our equipment,
> testing, and process controls.
>
> Joe Kane
> BAE SYSTEMS Controls
> Johnson City, NY
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|