TECHNET Archives

April 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Gregg Klawson <[log in to unmask]>
Date:
Fri, 23 Apr 2004 12:43:36 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Morse, Carrie" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Morse, Carrie" <[log in to unmask]>
Parts/Attachments:
text/plain (115 lines)
Wow,
Thanks to everyone for all the info.
I have a new update.  We tried 4 things based on a number of
recommendations:
1.  Applied flux and hit the area with an iron.  The discoloration went
away.  But, we have such a large area on so many boards there is no real
way to get this done in a timely fashion.  In addition, we scratched the
area up pretty well, so, either way, it looks bad.
2.  We tried to re-wave the board.  The discoloration got whiter/hazier
3.  Used Methyl Chloroform to test for permanency.  No mask was evident
on the swab which tells me the mask is cured.
4.  Lastly, we baked a board at 250F for 45 minutes -- no change.

So...Any ideas what it is or if it is detrimental?
Any suggestions?
It's Friday...If anyone can suggest the boards are OK and I can feel
comfortable to ship that would be fine by me.

-Carrie

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gregg Klawson
Sent: Friday, April 23, 2004 11:50 AM
To: [log in to unmask]
Subject: Re: [TN] White Discoloration -- Excessive Heat, Insufficiently
Cured SM, or, Both?

Carrie,

Some info from one SM mfr, this may help.

http://www.enthone.com/electronics/pdf/Imup5.pdf

-- Gregg

At 02:27 PM 4/22/2004, Morse, Carrie wrote:
>Here's the status.  I baked the boards for 45min @ 250F and...I still 
>have the white haze.  No change.  So, What do you all think?
>(IOW--HELP!!!!)
>
>-Carrie
>
>-----Original Message-----
>From: Brian Ellis [mailto:[log in to unmask]]
>Sent: Thursday, April 22, 2004 2:06 AM
>To: TechNet E-Mail Forum.; Morse, Carrie
>Subject: Re: [TN] White Discoloration -- Excessive Heat, Insufficiently

>Cured SM, or, Both?
>
>I'm not saying that this is the cause, but another possibility is 
>hydrolysis of the uncured solder mask. If the boards are coated and 
>then stored in a humid atmosphere before development (either before or 
>after
>exposure) for more than an hour or two, then some components in the 
>chemistry may absorb sufficient humidity to hydrolyse, partially 
>upsetting the polymerisation.
>
>I suggest methylene chloride would be better than acetone for a wipe 
>test, but it depends on the chemistry of the LPI.
>
>Brian
>
>Morse, Carrie wrote:
> > We are wave soldering a LPI board and seeing a Whitish Discoloration
> > -- Haze like -- only in the areas that the board has seen OA flux 
> > and
>wave.
> > We are using a wave pallet and the areas not exposed do not exhibit 
> > this phenomena.  This board is also processed through SMT for one 
> > side
>
> > and we do not see this around any of the SMT.
> >
> > We have not seen this problem in the past, and, the Wave operator 
> > states that the wave recipe has not changed.
> >
> > So, I am wondering -- if LPI is not fully cured, will it turn white 
> > when exposed to OA flux and Wave?
> > Also, what IS the max temp LPI should be able to see and for how 
> > long without discoloring?
> > We've done an Acetone test, but, it comes up clean and....I think I 
> > read in a previous posting that the Acetone may not be an effective 
> > test for LPI.  Is that true?  If so, What IS an effective test?
> >
> > I'm headed to the Omega tester to see "how clean" the board is.
> >
> > All advice is welcome!
> >
> > -Carrie
> >

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2