TechNetters:
I have a question on lead protrusion. We have ordered in components that
does not come through the PCB like it states in IPC-A-610C, 5.2.7.1,
figure 5-34. It is more along the L Min in the figure 5-34. Is this
acceptable for Class 2 manufacturing? I told my supervisor this is a
process indicator and should be corrected but he wants some more input and
so do I before we give the go ahead. Anxiously waiting.
Thanks
P. Lance Mayes
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
Mfg. Trainer