----- Original Message -----
From: "David Douthit" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, March 26, 2004 8:42 PM
Subject: Re: [TN] acyrlic coating deformed BGA balls
> For those of you following this thread I strongly recommend getting a
> copy of IPC-HDBK-830.
> The IPC committee worked for three years developing this document and it
> contains much of the information (plus a lot more) we have been
discussing.
>
> David A. Douthit
> Manager
> LoCan LLC
>
> Tegehall Per-Erik wrote:
>
> >Graham and David,
> >
> >I think you mix apples and pears regarding the "dustbag" issue. It is not
the low Tg per se that makes AR coatings susceptible to become "dustbags",
although it contributes. In contrast to epoxies, polyurethanes and
silicones, acrylics do not cure, they just dry. That is, no cross-linking
occurs between the acrylic molcular chains in the dryiong process. This is
the reason why acrylics are so easily dissolved in many solvents (and why
you can't have a solventless AR coating material). The absent of
cross-linking make it less rigid and allow it to "flow" and encapsulate
particles above Tg. A low Tg silicone coating will never do that even if the
Tg is much lower than for AR coatings. It is attractive to have a coating
that is easy to remove but the "dustbag" properties is one thing you have to
pay for it.
> >
> >Per-Erik Tegehall
> >IVF
> >
> >
> >-----Ursprungligt meddelande-----
> >Från: David Douthit [mailto:[log in to unmask]]
> >Skickat: den 26 mars 2004 04:30
> >Till: [log in to unmask]
> >Ämne: Re: [TN] acyrlic coating deformed BGA balls
> >
> >
> >
> >
> >>Graham,
> >>
> >>Welcome back. You must have enough frequent flyer miles to be part
> >>owner of British Airways.
> >>
> >>Here goes round two!
> >>
> >>Tg can be measured many different ways (up to 13 I believe).
> >>Each gives a slightly different reading. This generates a 3 to 5
> >>degree C "window" for Tg.
> >>Tg will also vary with moisture content (by as much as 5 degrees C).
> >>Also if the coating materials are a "mixture" it is impossible to
> >>attain a completely homogeneous mixture
> >>which will also create variations in Tg.
> >>
> >>For my use there is no single Tg but a "window"
> >>that can be as much as 10 degrees C wide.
> >>
> >>"So what"? you ask.
> >> Here is a material that has two different sets of physical properties
> >>depending on the temperature. The first problem is there is usually
> >>only one set of spec numbers issued with the product. This can be
> >>somewhat misleading.
> >>
> >>These coating materials are suppose to provide some form of a
> >>"barrier" that prevents
> >>malfunctions or disruption of the circuitry. Determining the
> >>"barrier'" effectiveness is very difficult.
> >>
> >>First, all polymers (coatings) are permeable to gases. Water vapor is
> >>one of many
> >>The rate of permeability varies with coating thickness and
> >>temperature. There is a
> >>dramatic increase in permeability when the Tg window is exceeded.
> >>There should be a requirement for coating vendors to provide
> >>permeability charts for there products.
> >>Some of these gases, such as Hydrogen Sulfide, are quite reactive.
> >>
> >>Second, there is Young's Modulus. This is the relative "stiffness" of
> >>the material.
> >>When the Tg window is exceeded there is a dramatic drop in The Young's
> >>Modulus.
> >>This is the "softening" of the material. In addition there is a
> >>dramatic rise in the CTE of the material.
> >>
> >>
> >
> > At some point above the Tg window the combination of reduced Young's
> >Modulus
> >
> >
> >
> >>and increasing expansion of the product allows solid particles
> >>deposited on the surface
> >>to "sink" into the coating. This results in a coagulated goo with
> >>virtually no barrier properties left at any temperature. I have seen
> >>this with the low Tg AR coatings.
> >>As near as I could figure this process began at about 40 degrees C.
> >>
> >>
> >>What makes this whole issue seriously difficult is that the
> >>"effective" life of the coating
> >>is primarily dependent on the type of atmospheric conditions it is
> >>exposed to.
> >>How fast the air is being exchanged at the surface determines the
> >>overall levels
> >>of exposure. I as mentioned in my response to Dewey changes in the
> >>industry are causing increased density, speed, and lower signal
> >>levels. This results in thermal problems with the hardware. Internal
> >>forced air cooling increases atmosphere exposure by up to 200 time
> >>over passive thermal exchanges. David Hillman mentioned some "ugly"
> >>situations I was involved in. These were a combination of internal
> >>forced air cooling and low Tg type AR coatings.
> >>I have determined that this combination is extremely risky.
> >>Understanding the critical role
> >>played by localized atmosphere exchanges is necessary when selecting
> >>coatings.
> >>
> >>High humidity > 60% is critical due to surface deposition of submicron
> >>particles and reactive gases. At this point an aqueous film > 5
> >>molecules thick can form. This film can dissolve
> >>salts and transport ions (leakage currents). There is also the fact
> >>that it is very acidic
> >>The National Association of Corrosion Engineers, NACE, has determined
> >>the Ph of these films to be between 2 and 3. The amount of time
> >>required to create this acidic film has
> >>been measured by Bell Labs at about 4 weeks in an office environment
> >>with the boards
> >>opened to the air.
> >>
> >>The combination of reactive gases/liquids, submicron particles,
> >>temperatures,
> >>humidity, and the and rate of atmospheric exchange will determine the
> >>life cycle of the coating barrier. Modern circuitry is rapidly
> >>becoming more sensitive to this combination.
> >>
> >>
> >
> >
> >
> >>Neither the mil standard nor the IPC guidelines address this
> >>combination. They are material qualification documents that insure
> >>certain minimum requirements are met. They are needed because there
> >>are more coating materials being sold then grains af sand on the beach
> >>that do not even meet these minimums (my favorites are the diluted
> >>"Super Glue" types).
> >>
> >>All this assumes that the board surface was "clean" at the time the
> >>coating was applied.
> >>If not, all bets are off!!
> >>
> >>The Mil specs and the IPC documents will not insure the coating will
> >>actually work for your
> >>end use environment. DO NOT BLINDLY EXCEPT THEM AS A GUARANTEE.
> >>
> >>
> >
> >
> >David A. Douthit
> >Manager
> >LoCan LLC
> >
> >
> >Graham Naisbitt wrote:
> >
> >
> >
> >>Hi everyone,
> >>
> >>I have been in France for the past couple of days, so did not respond to
> >>everyone earlier.....but here goes the duel! (You can't get rid of me
that
> >>easily!)
> >>
> >>The subject in question is David's oft repeated reference to low
Tg....and
> >>for the record the Tg of 1B31 is 14DegC not 15.
> >>
> >>So what?
> >>
> >>As Dewey said, and is no doubt backed-up in the Collins report submitted
by
> >>Dave Hillman, this is not necessarily a bad thing.
> >>
> >>Circuits exposed to wide temperature variations, coupled with high
levels of
> >>humidity are quite commonly conformally coated. The coating MUST
therefore
> >>be capable of surviving temperatures commonly down to -65DegC and up as
high
> >>as +125DegC or more.
> >>
> >>I have the distinct impression - and David please correct me if I am
wrong -
> >>that David thinks that an acrylic coating such as 1B31, permits external
> >>"stuff" to descend through the coating and hence onto the circuit
surface.
> >>Whilst this might be the case, there are most certainly many other
forces at
> >>work or conditions that must be considered and it is inappropriate to
> >>zone-in on one issue in isolation.
> >>
> >>Definition of Tg: The temperature at which an amorphous polymer changes
from
> >>a hard and relatively brittle condition to a viscous or rubbery
condition.
> >>
> >>A simplistic view of a material's glass transition temperature (Tg) is
the
> >>temperature below which molecules have very little mobility. On a larger
> >>scale, polymers are rigid and brittle below their glass transition
> >>temperature and elastic above it.
> >>
> >>The Space Shuttle Challenger disaster was caused by a rubber O-ring that
was
> >>below its glass transition temperature and thus could not flex
adequately to
> >>form a proper seal around one of the two solid rocket boosters.
> >>
> >>So how about a coating that has a high Tg, Would this be better David?
In a
> >>purely high temperature environment the answer would be a definite
maybe!
> >>However, below its Tg it is brittle, therefore the lower the temperature
the
> >>more brittle it becomes and hey presto - the coating shatters allowing
all
> >>that nasty stuff to get in through the cracks!
> >>
> >>So, as stated by Dewey: The key is to understand the end use environment
and
> >>choose the coating that has the widest processing window, tolerates
rework
> >>and functionally does the job.
> >>
> >>You will now have to excuse me for saying so, but this is the very
reason
> >>why we have so many different coatings in our range - "horses for
courses"
> >>or, as Dewey so poetically referred to it: We have a huge selection of
> >>quality Dust Bags whatever your needs - we even do latex but I don't
want to
> >>go there right now....
> >>
> >>TTFN everyone
> >>
> >>Graham Naisbitt - with a little (lot!) of help from Phil Kinner.
> >>
> >>
> >>
> >>
> >>
> >>>To all,
> >>>I thought for a moment we were going to have an old fashioned duel
between
> >>>David and Graham.It would have been a shame to loose all that intellect
and
> >>>humor in one fell swoop.We would have missed Graham, also( just kidding
> >>>Graham).
> >>>
> >>>
> >>>
> >>>
> >>>
> >>>
> >>---------------------------------------------------
> >>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> >>To unsubscribe, send a message to [log in to unmask] with following text
in
> >>the BODY (NOT the subject field): SIGNOFF Technet
> >>To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> >>To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> >>Search the archives of previous posts at:
http://listserv.ipc.org/archives
> >>Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> >>-----------------------------------------------------
> >>
> >>
> >>
> >>
> >>
> >>
> >
> >
> >---------------------------------------------------
> >Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> >To unsubscribe, send a message to [log in to unmask] with following text in
> >the BODY (NOT the subject field): SIGNOFF Technet
> >To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> >To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> >Search the archives of previous posts at:
http://listserv.ipc.org/archives
> >Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> >-----------------------------------------------------
> >
> >---------------------------------------------------
> >Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> >To unsubscribe, send a message to [log in to unmask] with following text in
> >the BODY (NOT the subject field): SIGNOFF Technet
> >To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> >To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> >Search the archives of previous posts at:
http://listserv.ipc.org/archives
> >Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> >-----------------------------------------------------
> >
> >
> >
> >
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|