TECHNET Archives

March 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Dehoyos, Ramon" <[log in to unmask]>
Date:
Wed, 31 Mar 2004 09:34:12 -0800
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (88 lines)
        Once the resin, rosin or other type of solder oxide  barrier coating material is hydrogenized it turns white and it is hard to remove ( leaving it on for a long time or baking boards without cleaning them before hand ).  The white residue sometimes diffuses into the porous parts. One of the ways is to mechanically remove it with a brush.  The forum consensus from previous posting is that if a board is going to be coated it needs to be cleaned to remove dust, oils, flux etc.
         Some one correct me if I am wrong, it is my understanding that no clean flux cleaning agents after becoming activated and removing the oxides from the leads,  barrels and pads they become inert. That is why they are no clean. It does not mean that the remaining rosin will stick to the coating. On the contrary. CC will only lay over the top of it.
        Regards,
        Ramon


> -----Original Message-----
> From: Brian Ellis [SMTP:[log in to unmask]]
> Sent: Wednesday, March 31, 2004 9:55 AM
> To:   [log in to unmask]
> Subject:      Re: [TN] White residue
>
> Doug's answer is 100% correct, you can, BUT ... should you? There is no
> cut and dried answer. This has already been discussed n* times on this
> forum and you would get far more info by searching through the archives
> than we could summarise in a short answer here. In brief, though not as
> brief as Doug, only YOU can answer the question, yourself, after
> conducting extensive tests and qualifying both your processes and
> materials. If you don't wish to do this, the best recommendation is
> don't coat on top of residues of any nature.
>
> Brian
>
> * where n is a large integer.
>
> Somtawin Pornpottanamas wrote:
>
> > Has anyone ever seen white contaminate ( like a crystal) on assembly
> > boards , between IC lead? I found white residue on  some board after
> > reflow . I try to clean by used IPA, flux removal solvent and also DI
> > water. But could not remove it. I also found that after we used the
> > solvent to clean, the white residue increase more.
> >
> > Our process used no clean . What is this residue?  What type of solvent
> > that should be use to clean flux residue when we have to rework or
> > Dedug?
> >
> >
> >
> > Thanks & Regards,
> >
> >
> >
> > Somtawin Pornpottanamas
> >
> > Material Engineer
> >
> > Kimball Electronics (Thailand)
> >
> > Tel. 038-401566  ext. 211
> >
> > Fax. 038-495029
> >
> >
> >
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following text in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at: http://listserv.ipc.org/archives
> > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> > -----------------------------------------------------
> >
> >
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315>
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2