TECHNET Archives

March 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet (E-mail)" <[log in to unmask]>
Date:
Wed, 17 Mar 2004 12:08:36 +0200
Reply-To:
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="windows-1251"
From:
Yordan Venev <[log in to unmask]>
Parts/Attachments:
text/plain (27 lines)
Hi TechNetters!

We face a problem with flux residues on the bottom (solder) side of the PCB
after wave-soldering. We have tried to clean only the bottom side since
(usually) we do not clean the PCB after assembling, but it is very hard and
nearly impossible task! The PWB is FR4 substrate and the flux we use is
alcohol based no-clean for foam. I cannot specify the solder mask as type,
but what is obvious is the shining smooth surface. I have a strong feeling
that for better performance in solder wave process the mask should have math
surface. What should I specify to the PWB manufacturer as solder mask type?
And yet could we optimize the process in some way to reduce or even avoid
such problems? We try to follow the flux manufacturer's instruction about
application, preheat and etc.

Best regards,
Yordan Venev

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2