Hi Steve,
A few years back, I solder connectors like that using
solder donuts from Alphametal and the result looks
pretty good. I believe you can custom order those
donut in array form that is the same array as each
connector. Don't forget to calculate the solder
volume (donut size- ID/OD and thickness) needed to
fill each of the hole.
Good luck.
Ted
--- Steve Gregory <[log in to unmask]> wrote:
> Mornin' All!
>
> One of the guys from our bid department asked me to
> come and look at a
> backplane we're bidding on, and tell him how we
> would solder it? I went and looked
> at it, and I'm not sure how we would. Go to
> http://www.stevezeva.homestead.com
> and take a look at Backplane Topside, Backplane
> Backside, and Backplane
> Backside Leads.
>
> The leads for all the connectors protrude at least a
> half inch or longer out
> the bottom of the board. I'm assuming they are that
> long because they get wire
> wrapped after the backplane is assembled. But how do
> you solder something
> like that? Some sort of dip solder pot? Drag solder?
> I don't think I'm going to
> be able to solder a board with leads that long in
> our Electra wave solder.
>
> I can tell board was mass soldered, and I'm thinking
> it was dipped somehow.
> Because you can see tiny little peaks on most of the
> lead tips that go straight
> up and down. Is there such thing as some sort of dip
> solder machine?
>
> Sorry for all the dumb questions, but I've never
> been around a backplane like
> this, and don't really know how something like this
> gets built.
>
> Thanks!
>
> -Steve Gregory-
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using
> LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of
> Technet send e-mail to [log in to unmask]: SET Technet
> NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts:
> send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
>
-----------------------------------------------------
__________________________________
Do you Yahoo!?
Yahoo! Search - Find what you’re looking for faster
http://search.yahoo.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|