Has anyone ever seen white contaminate ( like a crystal) on assembly
boards , between IC lead? I found white residue on some board after
reflow . I try to clean by used IPA, flux removal solvent and also DI
water. But could not remove it. I also found that after we used the
solvent to clean, the white residue increase more.
Our process used no clean . What is this residue? What type of solvent
that should be use to clean flux residue when we have to rework or
Dedug?
Thanks & Regards,
Somtawin Pornpottanamas
Material Engineer
Kimball Electronics (Thailand)
Tel. 038-401566 ext. 211
Fax. 038-495029
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------