I can verify that keyboard functionality can be restored after a coffee
accident using "domestic stuff". Being unaware of the Apple advise
I actually flushed first with warm solution of liquid Flash solution
(low foam low residue household detergent),
Rinsed under warm tap.
then final rinse using "DI" water from one of those jug things,
I dried using "DI" diluted surgical spirit (US speak: rubbing alcohol)
which is actually just iso-propanol and hot air blow from hair dryer.
Keyboard has worked well for 4 years since then with no problems
Caution this procedure does not remove paper clips, large biscuit crumbs
and some thing which I can't identify but is probably Green and Blacks
plain chocolate.
:)
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: Wednesday, March 10, 2004 12:21 PM
To: [log in to unmask]
Subject: Re: [TN] FW: [TN] Pros and Cons on Type UR vice Type AR
ConformalCoating
Which would be enough to make me lose all confidence in Apple Mac.
Dishwashers have water softeners which exchange calcium ions in youe
water with sodium ions. I, for one, would not wish to know that there
were trace quantities of hygroscopic and strongly ionic sodium
carbonate, sodium sulfate etc. on ANY electronics assembly.
Brian
Graham Naisbitt wrote:
> Hmmm, according to Apple Mac, I can put my keyboard into the
> dishwasher if I have such a spill - but am told DO NOT allow it to go
> through the drying cycle as it is too hot.
> --
> Regards Graham Naisbitt
>
> [log in to unmask]
>
> Cell: 079 6858 2121
> Office: +44 (0)1252 813706
>
> Concoat Limited - Engineering Reliability in Electronics
>
> NEW Additional Web address: www.conformalcoating.com
>
> www.concoat.co.uk www.concoatsystems.com
>
>
>
>>They won't - I know from experience. But, do you want to pay $50 for a
>>keyboard that will take spills, or $10 for one that won't?
>>
>>
>>>>>[log in to unmask] 03/09/04 01:54PM >>>
>>
>> Shouldn't PWA modules be protected from any liquid? We can not
>>expect a keyboard survive a coffee spill.
>> Ramon
>>
>>
>>>-----Original Message-----
>>>From: Randy Bock Sr. [SMTP:[log in to unmask]]
>>>Sent: Tuesday, March 09, 2004 12:48 PM
>>>To: [log in to unmask]
>>>Subject: Re: [TN] FW: [TN] Pros and Cons on Type UR vice Type AR
>>
>>Conformal Coating
>>
>>>Bug juice concetrate makes a good bright work cleaner. Turko
cleaner
>>>was the thing to clean with. Mixed with water did ok. Straight
>>>would turn your hands to wrinkled prunes.
>>>
>>>
>>>
>>>Randy Bock Sr.
>>>Quality Manager
>>>GMS Naugatuck
>>>(p) 203 720-3861
>>>(f) 203 729-5397
>>>(email) [log in to unmask]
>>>
>>>
>>>
>>>
>>>David Douthit <[log in to unmask]>
>>>Sent by: TechNet <[log in to unmask]>
>>>03/09/2004 12:29 PM
>>>Please respond to
>>>"TechNet E-Mail Forum." <[log in to unmask]>; Please respond to David
>>>Douthit <[log in to unmask]>
>>>
>>>
>>>To
>>>[log in to unmask]
>>>cc
>>>
>>>Subject
>>>Re: [TN] FW: [TN] Pros and Cons on Type UR vice Type AR Conformal
>>>Coating
>>>
>>>
>>>
>>>
>>>
>>>
>>>Ramon,
>>>
>>>You might be amazed at what cleaning crews use on the interior and
>>>exterior of aircraft.
>>>
>>>David A. Douthit
>>>Manager
>>>LoCan LLC
>>>
>>>Dehoyos, Ramon wrote:
>>>
>>>
>>>> Thanks for the correction.
>>>> Ramon
>>>>
>>>>
>>>>
>>>>
>>>>>-----Original Message-----
>>>>>From: Crepeau, Phil (Space Technology)
>>>>>Sent: Tuesday, March 09, 2004 10:44 AM
>>>>>To: Dehoyos, Ramon
>>>>>Subject: RE: [TN] FW: [TN] Pros and Cons on Type UR vice Type
AR
>>>>>
>>>>>
>>>>
>>>>Conformal Coating
>>>>
>>>>
>>>>
>>>>>i think you meant type ar not ur.
>>>>>
>>>>>-----Original Message-----
>>>>>From: Dehoyos, Ramon (NG)
>>>>>Sent: Tuesday, March 09, 2004 6:08 AM
>>>>>To: [log in to unmask]
>>>>>Subject: [TN] FW: [TN] Pros and Cons on Type UR vice Type AR
>>>>>Conformal Coating
>>>>>
>>>>>
>>>>> One of the disadvantages of UR coating is that it will not
>>>>>
>>>>>
>>>>
>>>>withstand
>>>>
>>>>
>>>>
>>>>>solvents. Besides boards in aircrafts that might be closed to the
>>>>>fuel tank or in automobile engine compartments, most boards are
>>>>>not in
>>>>>
>>>>>
>>>>
>>>>proximity
>>>>
>>>>
>>>>
>>>>>to fuels, acetone or alcohol. So UR is plenty good. It saves a lot
>>>>>of
>>>>>
>>>>>
>>>>
>>>>boards
>>>>
>>>>
>>>>
>>>>>from being damaged during rework due to the simplicity of removal.
>>>>> Regards,
>>>>> Ramon
>>>>>
>>>>>
>>>>>
>>>>>
>>>>>>-----Original Message-----
>>>>>>From: Dehoyos, Ramon
>>>>>>Sent: Tuesday, March 09, 2004 8:15 AM
>>>>>>To: [log in to unmask]
>>>>>>Subject: Re: [TN] Pros and Cons on Type UR vice Type AR
Conformal
>>>>>>
>>>>>>
>>>>>
>>>>>Coating
>>>>>
>>>>>
>>>>>
>>>>>> One thing to know is that AR can be coated to patch UR but
>>>>>> not
>>>>>>
>>>>>>
>>>>
>>>>the
>>>>
>>>>
>>>>
>>>>>>other way around. Patching AR with UR creates a mix that takes too
>>>>>>long
>>>>>>
>>>>>>
>>>>
>>>>to
>>>>
>>>>
>>>>
>>>>>>dry, stays soft. So to switch from UR to AR is recommended.
>>>>>> Regards,
>>>>>> Ramon
>>>>>>
>>>>>>
>>>>>>
>>>>>>
>>>>>>>-----Original Message-----
>>>>>>>From: - Bogert [SMTP:[log in to unmask]]
>>>>>>>Sent: Monday, March 08, 2004 4:55 PM
>>>>>>>To:
>>>>>>>Subject: [TN] Pros and Cons on Type UR vice Type AR
Conformal
>>>>>>>
>>>>>>>
>>>>>
>>>>>Coating
>>>>>
>>>>>
>>>>>
>>>>>>>As a Class 3 customer we are considering mandating transition
>>>>>>>from
>>>>>>>
>>>>>>>
>>>>
>>>>Type
>>>>
>>>>
>>>>
>>>>>UR
>>>>>
>>>>>
>>>>>
>>>>>>to Type AR conformal coating, to make it easier to replace failed
>>>>>>components. Are there any Class 3 users of Type AR coating? What
>>>>>>is
>>>>>>
>>>>>>
>>>>>
>>>>>track
>>>>>
>>>>>
>>>>>
>>>>>>record for using Type AR? Are there any compatibility issues with
>>>>>>
>>>>>>
>>>>
>>>>certain
>>>>
>>>>
>>>>
>>>>>>types of solder masks? Any input you have would help. Another
>>>>>>
>>>>>>
>>>>
>>>>advantage
>>>>
>>>>
>>>>
>>>>>>with AR would be for returned equipment. The OEM could remove all
>>>>>>the coating from an assembly using alcohol, then perform
>>>>>>
>>>>>>
>>>>>>
>>>>>>>---------------------------------------------------
>>>>>>>Technet Mail List provided as a service by IPC using LISTSERV
>>>>>>>1.8e To unsubscribe, send a message to [log in to unmask] with
>>>>>>>following text
>>>>>>>
>>>>>>>
>>>>>
>>>>>in
>>>>>
>>>>>
>>>>>
>>>>>>>the BODY (NOT the subject field): SIGNOFF Technet>
>>>>>>>To temporarily halt or (re-start) delivery of Technet send e-mail
>>>>>>>to
>>>>>>>
>>>>>>>
>>>>>>
>>>>>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>>>>
>>>>>>
>>>>>>
>>>>>>>To receive ONE mailing per day of all the posts: send e-mail to
>>>>>>>
>>>>>>>
>>>>>>
>>>>>>[log in to unmask]: SET Technet Digest
>>>>>>
>>>>>>
>>>>>>
>>>>>>>Search the archives of previous posts at:
>>>>>>>
>>>>>>>
>>>>>
>>>>>http://listserv.ipc.org/archives
>>>>>
>>>>>
>>>>>
>>>>>>>Please visit IPC web site
>>>>>>>
>>>>>>>
>>>>>
>>>>>http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>>>>
>>>>>
>>>>>
>>>>>>for additional information, or contact Keach Sasamori at
>>>>>>[log in to unmask]
>>>>>>
>>>>>>
>>>>
>>>>or
>>>>
>>>>
>>>>
>>>>>>847-509-9700 ext.5315
>>>>>>
>>>>>>
>>>>>>
>>>>>>>-----------------------------------------------------
>>>>>>>bed-of-nails testing to quickly identify failed components.
>>>>>>>
>>>>>>>
>>>>>>
>>>>>>---------------------------------------------------
>>>>>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>>>>>To unsubscribe, send a message to [log in to unmask] with following
>>>>>>text
>>>>>>
>>>>>>
>>>>
>>>>in
>>>>
>>>>
>>>>
>>>>>>the BODY (NOT the subject field): SIGNOFF Technet
>>>>>>To temporarily halt or (re-start) delivery of Technet send e-mail
>>>>>>to
>>>>>>
>>>>>>
>>>>>
>>>>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>>>
>>>>>
>>>>>
>>>>>>To receive ONE mailing per day of all the posts: send e-mail to
>>>>>>
>>>>>>
>>>>>
>>>>>[log in to unmask]: SET Technet Digest
>>>>>
>>>>>
>>>>>
>>>>>>Search the archives of previous posts at:
>>>>>>
>>>>>>
>>>>
>>>>http://listserv.ipc.org/archives
>>>>
>>>>
>>>>
>>>>>>Please visit IPC web site
>>>>>>
>>>>>>
>>>>
>>>>http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>>>
>>>>
>>>>
>>>>>for additional information, or contact Keach Sasamori at
>>>>>[log in to unmask]
>>>
>>>or
>>>
>>>>>847-509-9700 ext.5315
>>>>>
>>>>>
>>>>>
>>>>>>-----------------------------------------------------
>>>>>>
>>>>>>
>>>>>
>>>>>---------------------------------------------------
>>>>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e>
>>>>>To unsubscribe, send a message to [log in to unmask] with following
>>>>>text
>>>
>>>in
>>>
>>>>>the BODY (NOT the subject field): SIGNOFF Technet
>>>>>To temporarily halt or (re-start) delivery of Technet send e-mail
>>>>>to
>>>>>
>>>>>
>>>>
>>>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>>
>>>>
>>>>
>>>>>To receive ONE mailing per day of all the posts: send e-mail to
>>>>>
>>>>>
>>>>
>>>>[log in to unmask]: SET Technet Digest
>>>>
>>>>
>>>>
>>>>>Search the archives of previous posts at:
>>>
>>>http://listserv.ipc.org/archives
>>>
>>>>>Please visit IPC web site
>>>
>>>http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>>
>>>>>
>>>>for additional information, or contact Keach Sasamori at
>>>>[log in to unmask]
>>>
>>>or
>>>
>>>>847-509-9700 ext.5315
>>>>
>>>>
>>>>
>>>>>-----------------------------------------------------
>>>>>
>>>>>
>>>>
>>>>---------------------------------------------------
>>>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>>>To unsubscribe, send a message to [log in to unmask] with following
>>>>text in the BODY (NOT the subject field): SIGNOFF Technet To
>>>>temporarily halt or (re-start) delivery of Technet send e-mail to
>>>
>>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>
>>>>To receive ONE mailing per day of all the posts: send e-mail to
>>>
>>>[log in to unmask]: SET Technet Digest
>>>
>>>>Search the archives of previous posts at:
>>>
>>>http://listserv.ipc.org/archives
>>>
>>>>Please visit IPC web site
>>>
>>>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>>>information, or contact Keach Sasamori at [log in to unmask] or
>>>847-509-9700 ext.5315
>>>
>>>>-----------------------------------------------------
>>>>
>>>>
>>>>
>>>>
>>>
>>>
>>>---------------------------------------------------
>>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
>>>unsubscribe, send a message to [log in to unmask] with following text
>>>in the BODY (NOT the subject field): SIGNOFF Technet To temporarily
>>>halt or (re-start) delivery of Technet send e-mail to
>>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>To receive ONE mailing per day of all the posts: send e-mail to>
>>>[log in to unmask]: SET Technet Digest
>>>Search the archives of previous posts at:
>>>http://listserv.ipc.org/archives Please visit IPC web site
>>>http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>>for additional information, or contact Keach Sasamori at
[log in to unmask] or
>>>847-509-9700 ext.5315
>>>-----------------------------------------------------
>>>
>>>
>>>
>>>---------------------------------------------------
>>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
>>>unsubscribe, send a message to [log in to unmask] with following text
>>>in the BODY (NOT the subject field): SIGNOFF Technet To temporarily
>>>halt or (re-start) delivery of Technet send e-mail to
>>
>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>
>>>To receive ONE mailing per day of all the posts: send e-mail to
>>
>>[log in to unmask]: SET Technet Digest
>>
>>>Search the archives of previous posts at:
>>>http://listserv.ipc.org/archives Please visit IPC web site
>>>http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>
>>for additional information, or contact Keach Sasamori at
>>[log in to unmask] or 847-509-9700 ext.5315
>>
>>>-----------------------------------------------------
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
>>unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>>or (re-start) delivery of Technet send e-mail to
>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>To receive ONE mailing per day of all the posts: send e-mail to
>>[log in to unmask]: SET Technet Digest
>>Search the archives of previous posts at:
>>http://listserv.ipc.org/archives Please visit IPC web site
>>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>>information, or contact Keach Sasamori at [log in to unmask] or
>>847-509-9700 ext.5315
>>-----------------------------------------------------
>>
>>
>>**********************************************************************
>>This email and any files transmitted with it are confidential and
>>intended solely for the use of the individual or entity to whom they
>>are addressed. If you have received this email in error please notify
>>the system manager.
>>
>>This footnote also confirms that this email message has been swept for
>>the presence of computer viruses.
>>
>>www.hubbell.com - Hubbell Incorporated
>>**********************************************************************
>>
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
>>unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>>or (re-start) delivery of Technet send e-mail to
>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>To receive ONE mailing per day of all the posts: send e-mail to
>>[log in to unmask]: SET Technet Digest
>>Search the archives of previous posts at:
>>http://listserv.ipc.org/archives Please visit IPC web site
>>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>>information, or contact Keach Sasamori at [log in to unmask] or
>>847-509-9700 ext.5315
>>-----------------------------------------------------
>>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::
This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.
:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|