TECHNET Archives

March 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Reeves, Tim R." <[log in to unmask]>
Date:
Wed, 31 Mar 2004 16:12:19 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Jeffrey Bush <[log in to unmask]>
Parts/Attachments:
text/plain (85 lines)
I believe that glass etching, as a minimum to "frost" or micro etch the
glass is needed.  Sodium Bifloride and replaced some of the more
aggressive chemistries over the years, but anyone doing a good desmear
and certainly plasma needs to remove the glass left protruding.  It is
only on the order of .2 mil, but given the drive to refine the cu
plating processes to support the increasing densities, the copper
thickness in the barrel will be kept to a minimum.  Both desmear and
glass etch are critical to maintain a reliable copper barrel. 


Jeffrey Bush
Director, Quality Assurance and Technical Support

                          76 Technology Drive - POB 1890
                             Brattleboro, Vermont 05302-1890
                                Tel. 802.257.4571.21 Fax. 802.257.0011
                                    [log in to unmask]
                              http://www.vtcircuits.com	



-----Original Message-----
From: Reeves, Tim R. [mailto:[log in to unmask]] 
Sent: Wednesday, March 31, 2004 2:04 PM
To: [log in to unmask]
Subject: Re: [TN] Hole wall quality


Everyone is saying inadequate glass etch but few fabricators these days
are really using a glass etch. Drilling doesn't look good, but I'd say
it's over-aggressive desmear. That's why so much glass fiber protrusion.
Franklin, what was desmear condition? Alkaline permanganate? How long,
what temp.? One-pass or two? Is it ordinary FR-4, high Tg, or more high
performance material?  The plating definitely looks thin, based on
comparison with inner foil, whether it's 1 oz. or 1/2 oz.

Tim Reeves
Tyco Printed Circuit Group - Dallas Division


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Werner Engelmaier
Sent: Tuesday, March 30, 2004 9:08 AM
Subject: Re: Hole wall quality


Hi Franklin,
Whether or not these PWBs will give trouble in service depends on the
product appllication--o.k. for benign environments, likely to fail in
servere environments. The certainly are not the prettiest x-sections I
have seen--inadequate glass etch, some glass-fiber rip-out, l plating
rather thin---all resulting in stress risers in thin plating that is
thinner still localized.

Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting 7
Jasmine Run Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2