Hi Charles,
When you ask for deeper scoring you should be very aware that they don't
score too deep: we had a situation with Amphenol where we lost the tiebar
before we had the connector mounted onto the board, and we had to scrap
several of them (and these connectors were VERY expensive).
We have also worked with a tool that was made by Amphenol to break off the
tiebar, but the operators didn't like it very much because they couldn't
feel anymore what they were doing. And if the scoring is not deep enough
you'll end up with some ruined solder joints anyhow!
Regards,
Daan Terstegge
http://www.smtinfo.net
----- Original Message -----
From: "Charles Caswell" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, March 03, 2004 9:41 PM
Subject: Re: [TN] cutter for tie bars.
Why yes they are. And I thought the same thing, not deep enough. But not all
pins the same either.
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Wednesday, March 03, 2004 1:53 PM
To: [log in to unmask]
Subject: Re: [TN] cutter for tie bars.
Hi Charles!
Are they Amphenol connectors? I was having some of the same issues. After
looking closer at the connectors, and then ultimately sending one of the
connectors to Amphenol, I (we) discovered that the leads hadn't been scored
deep
enough for the tie bar to be separated cleanly.
-Steve Gregory-
> I am looking for cutters to remove the tie bar from a surface mount
> connector. I can find lots of them that would work but remember seeing a
> tool
> in a catalog that was especially for this. Anybody using something like
> this?
> The tie bars are not breaking as easily as I think they should , leaving
the
> pins looking kinda sorry.
> Thanks
>
> Charles Caswell
> The Big Kahuna
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|