TECHNET Archives

March 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Date:
Tue, 30 Mar 2004 08:47:20 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Yehuda Weisz - Netvision <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Yehuda Weisz - Netvision <[log in to unmask]>
Parts/Attachments:
text/plain (71 lines)
Franklin,
From what I can see in these microsections, I would point the finger towards
the chemical processes, mainly because the innerlayers on these images do no
present any evidence of rough drilling (although you did mention the
nailheading, and it would be good to put up an image of this).
I can see glass fibers protruding into the hole, very possibly because of
lack in glass etch (as Susan has pointed out).
In addition, you could look into your primary metallization process (you
didn't write what it was - electroless or some kind of "direct") or into the
current values of the electroplating.
I think it would help all of us understand if you could put some images of
the entire length of the hole - it does matter where you see the faults
(entrance vs. middle) and BTW - how thick is your board, how many holes were
drilled per drill,  what drill parameters, what board material ?


Regards,

Yehuda


Yehuda Weisz
Tel: (972)-3-6342045
Cel: (972)-53-556897
----- Original Message -----
From: "Franklin D Asbell" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, March 30, 2004 12:45 AM
Subject: [TN] Hole wall quality


> I've been asked to evaluate some images, hole wall plating defects, and
try to locate the cause.
>
> The information available to me are these are drilled 0.021" holes, they
were drilled one panel up, four panels total, and there was only one 0.021"
tool per spindle. The spindles were new or repoints. Upon evaluating the
bits nothing really jumped out as bad...another image not posted shows
excessive nailheading.
>
> I'm open to any and all comments...as well as a list of items I can begin
checking...thanks
>
> I've posted the images at http://asbell.net/images.htm
>
> Franklin
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2