Wee,
Why are you using 1B31, with a Tg of 15 degrees C??
If this product is staying in an "office" environment then it may work.
For anything else it is very problematic!!
At room temperature, about 25 degrees C, there will be problems with
cold flow so the CTE doesn't matter (it's too soft!).
David A. Douthit
Manager
LoCan LLC
Lum Wee Mei wrote:
> Hello,
>
> My colleague coated several test boards using 1B31 through brushing that
> have BGAs moutned on them. When he took some X-rays on them, he found
> many balls are deformed with what he termed as "cauliflowers" like
> patterns on the balls. He attributed the casue to the CTE difference of
> the acrylic coating. Is that possible?
>
> I will try to get the X-rays from him and post it to steve so that you
> experts out there can provide a second opinion on this "cute"
> observation. Meanwhile, hope some of you can share your experience with
> BGAs and 1B31 coating.
>
> Thanks and regards,
> Wee Mei
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|