TECHNET Archives

March 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Fri, 19 Mar 2004 10:40:58 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Creswick, Steven" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Creswick, Steven" <[log in to unmask]>
Parts/Attachments:
text/plain (148 lines)
Mike,

You might also consider Sikama.  Their units are conduction and/or convection (depending on the unit) and can usually be equipped for inert atmosphere.  Not sure if they are small enough for you, however.

Not sure if it is what you want, but here is a contact.  Just give Marc a call.

Marc Aldecoa
Sales Manager
Sikama International, Inc
PH 805 962 1000 x100
[log in to unmask]

http://www.sikama.com


Steve Creswick - Gentex Corporation


-----Original Message-----
From: Jason W. Gregory [mailto:[log in to unmask]]
Sent: Friday, March 19, 2004 9:07 AM
To: [log in to unmask]
Subject: Re: [TN] Batch Reflow Ovens


Ramon,

you didn't mention the company name. Please Email me off-line for that
info.


Jason Gregory
Manufacturing Engineer
LaBarge Inc. --- Houston
(281)207-1464
(281)207-1435 fax
(832)724-0076 cell
[log in to unmask]
http://www.labarge.com





                      "Dehoyos, Ramon"
                      <ramon.dehoyos@NG        To:       [log in to unmask]
                      C.COM>                   cc:
                      Sent by: TechNet         Subject:  Re: [TN] Batch Reflow Ovens
                      <[log in to unmask]>


                      03/19/2004 07:33
                      AM
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to
                      "Dehoyos, Ramon"






        Mike:
        I have been doing what you are doing and found this company. They
even gave me a list of customer to get their opinion from. They seem to
have a good record based on their customers. Their prices are very
reasonable.
        Regards,
        Ramon

> -----Original Message-----
> From: Mcmaster, Michael [SMTP:[log in to unmask]]
> Sent: Thursday, March 18, 2004 3:04 PM
> To:   [log in to unmask]
> Subject:      [TN] Batch Reflow Ovens
>
> I'm looking into purchasing a small benchtop reflow oven.  Not sure at
this
> point if it's going to be batch or conveyorized.
>
> I'd use it for sweat soldering pallets and heat sinks to PWBs.  Ideally
I'd
> like something capable of doing reflow of lead free solder on a  12x12
> board.
>
> I'd appreciate any recommendations or experience with different
> models/manufacturers equipment.  Feel free to contact me off line.
>
> Thanks in advance for your help.
>
> Mike McMaster
> RF Product Engineer
> Merix Corporation
> 503-992-4263
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2