Mike,
I have used a batch reflow oven (model #GF-B) from a company called Automated
Production Systems. Check it out at
http://www.apsgold.com/pdf_public/gf12bro.pdf. I mainly used it to assemble prototype PCB's that used BGA type
components. I used it to both assemble and rework the boards. It has a shelf area of ~
12" x 12" which just met our needs.
Initially, I had to play around with it for a bit to determine how well it
moved the temperature. But using a hand held temperature meter with a couple of
thermocouple inputs helped me to set up my required thermal cycle for the
boards that I was working with. I hope this info helps.
Regards,
Bob Walker
[log in to unmask]
In a message dated 3/18/2004 3:04:33 PM Eastern Standard Time,
[log in to unmask] writes:
I'm looking into purchasing a small benchtop reflow oven. Not sure at this
point if it's going to be batch or conveyorized.
I'd use it for sweat soldering pallets and heat sinks to PWBs. Ideally I'd
like something capable of doing reflow of lead free solder on a 12x12
board.
I'd appreciate any recommendations or experience with different
models/manufacturers equipment. Feel free to contact me off line.
Thanks in advance for your help.
Mike McMaster
RF Product Engineer
Merix Corporation
503-992-4263
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------