TECHNET Archives

March 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 18 Mar 2004 16:34:57 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="UTF-8"
From:
Edwin Louis <[log in to unmask]>
Parts/Attachments:
text/plain (137 lines)
Is anyone getting reliability with Alloy 42 leaded TSOPs on Thurmount PWBs
and if so what are the drawbacks?

-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Thursday, March 18, 2004 9:01 AM
To: [log in to unmask]
Subject: Re: [TN] TSOPs


Royce,
I realize why you do that from a PROCESS point of view, but Edwin, Werner
and I were talking in terms of RELIABILITY.
Bev

-----Original Message-----
From: Taylor, Royce [mailto:[log in to unmask]]
Sent: March 18, 2004 8:55 AM
To: [log in to unmask]
Subject: Re: [TN] TSOPs


We have one customer that has more than one assembly with TSOPS utilizing
alloy 42 (TI parts I believe). For these assemblies I run my Peak relow
temps higher than I normally do (220-230 C.) with good results.

Royce
*************************************************************************
Royce Taylor
Process Engineering/Production
Suntron Corporation NEO
104 Glenn Street
Lawrence, MA 01843
(978)747-2061 voice
(978)747-2010 fax
[log in to unmask]



-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Thursday, March 18, 2004 8:25 AM
To: [log in to unmask]
Subject: Re: [TN] TSOPs


Edwin,
Good for you for using the archives!  Short answer: yes, rejected!
Bev Christian
Research in Motion

-----Original Message-----
From: Edwin Louis [mailto:[log in to unmask]]
Sent: March 18, 2004 8:21 AM
To: [log in to unmask]
Subject: Re: [TN] TSOPs


I notice in the IPC Archives that all of the questions and comments about
alloy 42 were in the
~1994-1995 time period. Has the general population out there totally
rejected TSOPS
with alloy 42 leads? No comments or questions appear from 2001 to present.

-----Original Message-----
From: Werner Engelmaier [mailto:[log in to unmask]]
Sent: Tuesday, March 16, 2004 6:43 AM
To: [log in to unmask]
Subject: Re: [TN] TSOPs


Hi Edwin,
>Are there any specifications ,standards or articles on soldering TSOPs
>especially ones with Alloy42 leads?
There are some papers:
Engelmaier, W., "Alloy 42--Not a Choice Material for Surface Mount Leads," 
35th Annual IPC Meeting, Bal Harbour, FL, April 1992.  
Engelmaier, W., and B. Fuentes, "Alloy 42: A Material to be Avoided for 
Surface Mount Solder Component Leads and Lead Frames," Proc. Surface Mount 
International Conf., San Jose, CA, August-September 1994, pp. 644-655; also
in Proc. 
Int. Electronics Packaging Conf. (IEPS), Atlanta, September 1994, pp.
503-516; 
also in Proc. 19th Ann. Electronics Manufacturing Sem., Naval Air Warfare 
Center, China Lake, CA, February 1995, pp. 5-20; also in Proc. NEPCON West
‘95, 
Anaheim, CA, February-March 1995, pp. 385-395; also in Soldering & Surface
Mount 
Technology, No. 21, October 1995, pp. 20-25.  

Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL  32174  USA
Phone: 386-437-8747, Fax: 386-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2