All plating is a "donation" of electrons to the metal ions in solution to
turn them from charged ions to the metal form.
In electroplating, the electrons are pumped to the work being plated by the
rectifier. In electroless plating, the electrons are donated by another
chemical in solution...formaldehyde, or hypophosphite. In immersion plating, the
substrate metal dissolves, and in the process gives up electrons, which transfer
to the metal being plated out.
In your case you have exposed Copper or Nickle going into solution, and
giving up electrons in the process, and their electrons are transferred to the Gold
by the Copper traces, where they react with the Silver in solution...and
voila! Magic!
Is this clearer?
Rudy Sedlak
RD Chemical Company
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|