For this problem, we have tried the following. it has given us some
improvement,
1. Normal Solder mask process
2. Final cure boards
3. UV bump at 1200 mj, the two sides of the board.
Any further suggestions ?
|---------+---------------------------->
| | Eddie Rocha |
| | <[log in to unmask]
| | M> |
| | Sent by: TechNet |
| | <[log in to unmask]>|
| | |
| | |
| | 03/11/2004 05:38 |
| | AM |
| | Please respond to|
| | EddieR |
| | |
|---------+---------------------------->
>--------------------------------------------------------------------------------------------------------------|
| |
| To: [log in to unmask] |
| cc: (bcc: Parial Swati/NAN/ATS/IN) |
| Subject: Re: [TN] The Sin of Tin -- Again |
>--------------------------------------------------------------------------------------------------------------|
The tin process is aggressive on soldermask and if the surface of a
PCB is not prep'd properly before applying the soldermask, the tin
process will show this. The tin process is not usually the culprit in
this case. It's the soldermask process.
On 10 Mar 2004 at 15:39, Morse, Carrie wrote:
We have some unpopulated bare boards that are white tin plated with
SMOBC. The boards are exhibiting peeling mask at the interface between
the tin pad (TH and SMT) and the mask along the circuit runs. Per
IPC
A610 , exposed copper is not acceptable in this case. Can anyone
provide possible root causes to this phenomena? The boards are
date
coded from Oct 2003 as well as Feb 2004. Both lots exhibit the
exposed
copper/missing mask. These boards were also stored in a
Temp/RH of
about 70F/10-15%RH
TIA
-Carrie
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV
1.8e
To unsubscribe, send a message to [log in to unmask] with
following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-
509-9700 ext.5315
-----------------------------------------------------
-- Thanks,
Eddie Rocha
(408) 978-8992 x 282
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
Scan by AT&S virus protection
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|