Hans, All,
We use both AR and UR in different applications on Class 3. It really
depends on your end use and fitness for use, and in particular the unit or
requirement specification you are trying to meet. AR is easier to rework
etc, bit that also means it can be less effective when it comes to
protection... tougher coating = generally harder to remove.
If you have a requirement to protect against aircraft fluids etc, then AR
will be a poorer choice. If you want to use it in a telephone box, AR will
do a great job. AR does however have better moisture properties than UR.
None of course are truly hermetic, but they will do well in a
condensation/evaporation scenario.
AR may be good for rework (if/when it is needed), but it also needs to be
good for service, which may be decades.
Clive ff.
-----Original Message-----
From: Hinners Hans M Civ WRALC/LUGE [mailto:[log in to unmask]]
Sent: 09 March 2004 15:00
To: [log in to unmask]
Subject: Re: [TN] Pros and Cons on Type UR vice Type AR Conformal
Coating
*** WARNING ***
This mail has originated outside your organization,
either from an external partner or the Global Internet.
Keep this in mind if you answer this message.
I've approved switching from UR to AR at the request of the repair line. The
assemblies are IPC-A-610 Class 3, on aircraft,crew accessible cargo area.
Hans
~~~~~~~~~~~~~~~
Hans M Hinners
AC-130 Systems Engineer
WR-ALC/LUGE
Special Operations Forces / Combat Search & Rescue
System Program Office
226 Cochran St
Robins AFB, GA 31098
DSN Prefix: 468
Com: (478) 926 - 5847
Fax: (478) 926 - 4911
mailto:[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Tuesday, March 09, 2004 8:15 AM
To: [log in to unmask]
Subject: Re: [TN] Pros and Cons on Type UR vice Type AR Conformal Coating
One thing to know is that AR can be coated to patch UR but not the
other way around. Patching AR with UR creates a mix that takes too long to
dry, stays soft. So to switch from UR to AR is recommended.
Regards,
Ramon
> -----Original Message-----
> From: - Bogert [SMTP:[log in to unmask]]
> Sent: Monday, March 08, 2004 4:55 PM
> To: [log in to unmask]
> Subject: [TN] Pros and Cons on Type UR vice Type AR Conformal Coating
>
> As a Class 3 customer we are considering mandating transition from
> Type UR
to Type AR conformal coating, to make it easier to replace failed
components. Are there any Class 3 users of Type AR coating? What is track
record for using Type AR? Are there any compatibility issues with certain
types of solder masks? Any input you have would help. Another advantage
with AR would be for returned equipment. The OEM could remove all the
coating from an assembly using alcohol, then perform
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
> bed-of-nails testing to quickly identify failed components.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or
distribute its contents to any other person.
********************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|