TECHNET Archives

March 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Kane, Joseph E" <[log in to unmask]>
Date:
Mon, 8 Mar 2004 17:27:58 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Douthit <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii; format=flowed
From:
David Douthit <[log in to unmask]>
Parts/Attachments:
text/plain (108 lines)
Joseph,

I am not particularly fond of AR type coatings for class 3 products for
the following reasons:

1. Low Tg,  from 15 to 40 degrees C
2.  As mentioned most forms of hydrocarbon based solvent (and their
fumes) can desolve/liquidfy
     the coating.

Depending on the end use environment these items can pose serious problems!

I suggest you get a copy of the IPC-HDBK-830 (Conformal Coating
Handbook) before you decide.

David A. Douthit
Manager
LoCan LLC




Kane, Joseph E wrote:

>We're Class 3, mostly military aircraft electronics.
>Historically, we've used Type UR, but we've recently
>brought in some work from another plant that has
>been using acrylic.  We're in the process of switching
>everything over to our UV-curable urethane for the
>following reasons:
>
>1. UV-curing saves a whole lot of cycle time.  The
>acrylic must be air-dried or baked.
>
>2. In order to perform any rework at all, you must be
>very careful when removing coating in particular spots,
>and things can look pretty ugly after recoating.  More
>often than not, we end up stripping and re-coating the
>whole thing.  More lost time.
>
>3. Some of our designs require solvent-resistant coating.
>If we're going to settle on one type of coating, it might
>as well be urethane.
>
>For the record, we haven't noticed any compatibility
>issues with the fluxes and solder masks that we've been
>using.
>
>Of course, YMMV.  If you're doing occasional touchup on
>a solder joint or two, Type UR may be preferred.  If you
>need to replace a lot of components, it's probably easier
>to strip the coating and start over.
>
>-Joe
>
>-----Original Message-----
>From: - Bogert [mailto:[log in to unmask]]
>Sent: Monday, March 08, 2004 4:55 PM
>To: [log in to unmask]
>Subject: [TN] Pros and Cons on Type UR vice Type AR Conformal Coating
>
>
>As a Class 3 customer we are considering mandating transition from Type UR
>to Type AR conformal coating, to make it easier to replace failed
>components.  Are there any Class 3 users of Type AR coating?  What is track
>record for using Type AR?  Are there any compatibility issues with certain
>types of solder masks?  Any input you have would help.  Another advantage
>with AR would be for returned equipment.  The OEM could remove all the
>coating from an assembly using alcohol, then perform
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>-----------------------------------------------------
>bed-of-nails testing to quickly identify failed components.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
>-----------------------------------------------------
>
>
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2