Lance: Try using non metal wrist straps.
Regards,
Ramon
> -----Original Message-----
> From: Lance Mayes [SMTP:[log in to unmask]]
> Sent: Thursday, February 26, 2004 12:08 PM
> To: [log in to unmask]
> Subject: [TN] Allergies to ESD Wriststraps
> Importance: High
>
> Hello everybody;
>
> We've been experiencing a problem with one of our employees. She has a
> rash that develops when she wears the ESD writs straps.
> When the metal comes in contact with her skin the rash shows up within a
> few hours. Are there any good remedies or has any one had this problem
> before? Anything would be appreciated.
>
> Thanks
>
> P. Lance Mayes
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
> Mfg. Trainer
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------