Hi Yannick,
Water soluble paste and the alloy mixture of the paste and/or BGA have
nothing to do with each other. Water soluble is talking about the flux
vehicle of the solder pastes (the non-metal stuff in the solder paste).
2% silver alloy solder paste is absolutely compatible with BGA.
Water soluble flux is compatible with BGA, but your cleaning equipment
may not be compatible with BGA. Water soluble flux residue must be
cleaned off the PCB very well or you are very likely to have
electromigration failures after some time in the field. If the BGA ball
diameter is 0.030" or larger, most modern in-line aqueous cleaners do a
fine job. When you get to 0.013" diameter BGA balls, cleaning life
becomes difficult, (but not impossible). Anything in-between and clean
ability just depends.
Ryan Grant
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Yannick Brisson
Sent: Tuesday, February 24, 2004 2:47 PM
To: [log in to unmask]
Subject: [TN] BGA and Water solube paste
Hi,
Somebody here just ask me something about BGA and water soluble
paste. He wants to know if water soluble and BGA could work together.
Most
of the BGA avec a ball of 63/37 and water soluble can have the same
composition too but some have 2 Ag in it. Can it be compatible? What
about
the flux?
Thank you
Yannick
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|