I am assuming that you want a dye which "glows" under black light? If this
is the case, what you want is commonly used in typical laundry detergents as
"optical brighteners", to make clothes look cleaner...
And, we have some of this sort of dye in our arsenal of raw materials.. the
amount you will need is so small, it is trivial, and can be put into a normal
business envelope and mailed to you. And that is exactly what I am offering to
do. Tell me how much flux you want to dye, and I will send you the dye
required, at no charge.
Rudy Sedlak
RD Chemical Company
650-962-8004
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|