<< What are the "standard" thicknesses for double-sided boards? >>
Traditionally, boards were in fractions of an inch - 62 mils or ".062" is the
traditional 1/16 inch thickness for two sided laminate. As McDonalds says -
Billions sold.
Denny Fritz
MacDermid
---------------------------------------------------