If the standard material is .044", including the copper, how would I call it
out using the IPC-4101 designation?
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
-----Original Message-----
From: Roger Stoops [SMTP:[log in to unmask]]
Sent: Thursday, February 12, 2004 3:33 PM
To: TechNet E-Mail Forum.; Marsico, James
Subject: RE: [TN] FR-4 standard thickness
Yes, but vendors call it .044", 6 layers of 7628 laminate (what's a
mil between friends, anyway?). This is a nominal number, and typically
includes the copper thickness.
They may want to consider calling out .044" to reduce confusion.
Here's a link for Nan-Ya Plastics Electronic Mat'l Div. as an
example:
http://www.npc.com.tw/Emd-e/fr-div1.htm
Roger M. Stoops, CID+
Trimble Navigation Ltd., Dayton, OH, USA
Ph: +01 937.245.5288
Fax: +01 937.233.7511
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Marsico, James
Sent: Thursday, February 12, 2004 3:04 PM
To: [log in to unmask]
Subject: [TN] FR-4 standard thickness
Good day Technet:
Our designers are designing a PWB using IPC 4101/24 (FR406) material
that's
.045" thick. Is this a standard thickness that is readily
available?
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|