TECHNET Archives

February 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 5 Feb 2004 10:37:33 EST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Rudy Sedlak <[log in to unmask]>
Parts/Attachments:
text/plain (35 lines)
Gunter:

I want to give you a short description of plating here, so you can be sure
you are asking the right question.  All plating involves transferring electrons
to the ion in the plating bath to cause it to become a metal, instead of an
ion.  There are three kinds of plating, the difference in the 3 different kinds
is where the electron come from.

In Electrolytic plating, the electron is supplied by a rectifier, also known
as an "electron pump".

In Electroless plating, the electron is supplied by a chemical in the plating
bath, also known as "a reducing agent", typical being formaldehyde, or
Hypophosphite.

In immersion, (also know as Galvanic plating, after Mr. Galvanos, who
invented it, even before Brian was born!) the electron comes the substrate being
plated.  The substrate metal is dissolved, and as it does, it donates electrons,
which transfer to the metal being plated.

In your question, do you mean immersion/galvanic plating, or electroless
plating?

Rudy Sedlak

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2