I would strongly advise a filter loop. This product is not a
conventional saponifier. I suspect it forms large micelles round
hydrophobic molecules from the flux residues and, if these are filtered
out, it keeps the solution clean for a lot longer and prevents the
re-depositing of particles onto the assemblies (and probably clogging).
Our experience with filtration was quite positive.
I agree going water-soluble will give you probably better results at a
lot less expenditure, providing you have good process control.
The operating manual, containing a large amount of technical detail on
Vigon cleaning, of the machine I made is at
http://www.protonique.com/apl5special/protonique_sa.htm
NB This may appear commercial but I excuse myself as this machine is no
longer made and the company has been long liquidated.
Brian
Kane, Joseph E wrote:
> We're using Vigon A-200 in a Technical Devices in-line
> system, cleaning RMA flux residues. The wash section has
> two pumps, one for high pressure spray, and one for high
> volume/flood. We successfully clean a wide range of
> assembly types at 1.5 feet per minute.
>
> We're in the process of changing to a water-soluble flux
> for wave solder, and a "cleanable" no-clean paste for SMT.
> Some product will stay with RMA.
>
> Vigon is expensive, but the major advantage is that you
> may not need to dump the wash tank for a good long while
> (months). Of course, this reduces chemistry and disposal
> costs. We use deionized water for makeup, keep solution
> concentration between 15 and 18%, and the tank at 122F.
> We stupidly tried makeup with city water once, and developed
> a foaming problem.
>
> We don't have a filter loop - larger particles seem to stay
> in the bottom of the tank. We're thinking about adding a
> filter loop to see if this would reduce clogging in the
> spray nozzles.
>
> -Joe
>
>
> -----Original Message-----
> From: Brian Ellis [mailto:[log in to unmask]]
> Sent: Wednesday, February 18, 2004 2:36 AM
> To: [log in to unmask]
> Subject: Re: [TN] Cleaning Chemistry
>
>
> Yes, I designed a batch cleaning machine specifically for Vigon. The
> important thing is to keep the filter circuit pump running 24/24 or, at
> least, several hours after use. The disagreeable part is changing the
> filters because the saponifier solution is quite alkaline and the spent
> filters are hazardous waste. I recommend you have 2 sets of filters and
> a pair of 3-way valves, with a pressure gauge on the pipe between the
> pump and the valve, so that you can see when a filter is becoming
> clogged. I did toy with backwashing the filter but I don't think that
> this would make much difference.
>
> When discarding used Vigon solution, remember that it, too, is alkaline
> hazardous waste, containing heavy metals and toxic hydrocarbons. If sent
> to a specialist company for disposal, the containers must be
> appropriately labelled.
>
> The Vigon itself worked well with some fluxes and pastes, but not all.
> As with all processes, qualification of the flux/paste, in conjunction
> with Vigon, **under YOUR particular conditions of use**, is essential.
>
> Brian
>
> Dehoyos, Ramon wrote:
>
>> Hi Yo'all:
>> One of our board vendors has changed their cleaning agent
>
> to
>
>>Vigon A 200 for their in line cleaning. Their in line cleaner is an
>>Electrovert Aquastorm. Does anybody have any experience with this agent?
>>Vigon A 200 is suppossed to be good for medium to high pressure.
>> TIA.
>> Ramon
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to
>
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>
>>To receive ONE mailing per day of all the posts: send e-mail to
>
> [log in to unmask]: SET Technet Digest
>
>>Search the archives of previous posts at: http://listserv.ipc.org/archives
>>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
>
>>-----------------------------------------------------
>>
>>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|